Perovskite/Colloidal Quantum Dot Tandem Solar Cells: Theoretical Modeling and Monolithic Structure AITranslate

University of Cambridge; University of Cambridge; Linköping University;Centre for Nanophotonics; University of Oxford;Centre for Nanophotonics; University of Cambridge; University of Cambridge
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal-halide perovskite-based tandem solar cells show great promise for overcoming the Shockley–Queisser single-junction efficiency limit via low-cost tandem structures, but so far, they employ conventional bottom-cell materials that require stringent processing conditions. Meanwhile, difficulty in achieving low-bandgap (<1.1 eV) perovskites limits all-perovskite tandem cell development. Here we propose a tandem cell design based on a halide perovskite top cell and a chalcogenide colloidal quantum dot (CQD) bottom cell, where both materials provide bandgap tunability and solution processability. A theoretical efficiency of 43% is calculated for tandem-cell bandgap combinations of 1.55 (perovskite) and 1.0 eV (CQDs) under 1-sun illumination. We highlight that intersubcell radiative coupling contributes significantly (>11% absolute gain) to the ultimate efficiency via photon recycling. We report an initial experimental demonstration of a solution-processed monolithic perovskite/CQD tandem solar cell, showing evidence for subcell voltage addition. We model that a power conversion efficiency of 29.7% is possible by combining state-of-the-art perovskite and CQD solar cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00207

Chinese Library Classification Number:

Citation Information:

Metal-halide perovskite-based tandem solar cells show great promise for overcoming the Shockley–Queisser single-junction efficiency limit via low-cost tandem structures, but so far, they employ conventional bottom-cell materials that require stringent processing conditions. Meanwhile, difficulty in achieving low-bandgap (<1.1 eV) perovskites limits all-perovskite tandem cell development. Here we propose a tandem cell design based on a halide perovskite top cell and a chalcogenide colloidal quantum dot (CQD) bottom cell, where both materials provide bandgap tunability and solution processability. A theoretical efficiency of 43% is calculated for tandem-cell bandgap combinations of 1.55 (perovskite) and 1.0 eV (CQDs) under 1-sun illumination. We highlight that intersubcell radiative coupling contributes significantly (>11% absolute gain) to the ultimate efficiency via photon recycling. We report an initial experimental demonstration of a solution-processed monolithic perovskite/CQD tandem solar cell, showing evidence for subcell voltage addition. We model that a power conversion efficiency of 29.7% is possible by combining state-of-the-art perovskite and CQD solar cells.

quote

GB/T 7714-2015 [1] Arfa Karani, Le Yang, Sai Bai, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00207.
MLA [1] Arfa Karani, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00207.
APA [1] Arfa Karani, Le Yang, Sai Bai, Moritz H. Futscher, Henry J. Snaith, Bruno Ehrler, Neil C. Greenham, & Dawei Di. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00207
IEEE [1] Arfa Karani, Le Yang, Sai Bai, Moritz H. Futscher, Henry J. Snaith, Bruno Ehrler, Neil C. Greenham, and Dawei Di, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00207.