Molecular dynamics simulation study on cross-type graphene resonator AITranslate

Semyung University; Chung-Ang University; Korea National University of Transportation
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • We present resonator schematics based on a cross-type graphene. • Cross-type graphene-resonator can detect the variations in two-dimension. • Detecting the polarization of the zigzag or armchair directions. The resonators based on graphene nanoribbon have been of interest for a building block to develop electro-mechanical devices on a nanometer scale. Here, we present resonator schematics based on a cross-type graphene and investigate its dynamic features via classical molecular dynamics simulations. This cross-type graphene-resonator can detect the tension and electrical variations in two-dimension. Our simulation results showed that the cross-type graphene-resonator exhibits great potential in the applications to detect the polarization of the zigzag or armchair directions, because its oscillation dynamics are electromechanically coupled and its electronic states directionally depend on the edge structures by controlling the widths of the zigzag and the armchair edges. The deflective motions of the cross-type graphene-resonator under the driving forces were very similar to those of the graphene-nanoribbon resonator.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.09.053

Chinese Library Classification Number:

Citation Information:

Highlights • We present resonator schematics based on a cross-type graphene. • Cross-type graphene-resonator can detect the variations in two-dimension. • Detecting the polarization of the zigzag or armchair directions. The resonators based on graphene nanoribbon have been of interest for a building block to develop electro-mechanical devices on a nanometer scale. Here, we present resonator schematics based on a cross-type graphene and investigate its dynamic features via classical molecular dynamics simulations. This cross-type graphene-resonator can detect the tension and electrical variations in two-dimension. Our simulation results showed that the cross-type graphene-resonator exhibits great potential in the applications to detect the polarization of the zigzag or armchair directions, because its oscillation dynamics are electromechanically coupled and its electronic states directionally depend on the edge structures by controlling the widths of the zigzag and the armchair edges. The deflective motions of the cross-type graphene-resonator under the driving forces were very similar to those of the graphene-nanoribbon resonator.

quote

GB/T 7714-2015 [1] Oh Kuen Kwon, Ho Jung Hwang, Jeong Won Kang. Computational Materials Science, 2014(82). DOI:10.1016/j.commatsci.2013.09.053.
MLA [1] Oh Kuen Kwon, et al., Computational Materials Science, no. 82, 2014, https://doi.org/10.1016/j.commatsci.2013.09.053.
APA [1] Oh Kuen Kwon, Ho Jung Hwang, & Jeong Won Kang. (2014). Computational Materials Science(82). https://doi.org/10.1016/j.commatsci.2013.09.053
IEEE [1] Oh Kuen Kwon, Ho Jung Hwang, and Jeong Won Kang, Computational Materials Science, no. 82, 2014, doi: 10.1016/j.commatsci.2013.09.053.