Triptycene, Phenolic-OH, and Azo-Functionalized Porous Organic Polymers: Efficient and Selective CO2 Capture AITranslate

Indian Institute of Technology Patna; Indian Institute of Technology Patna; Indian Institute of Technology Patna; Indian Institute of Technology Patna
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The well-known azo coupling reaction was utilized to yield a new group of triptycene-derived azo polymers (TAPs) bearing phloroglucinol units. TAPs have hierarchical porosity (presence of micropores and mesopores) and are thermally stable. TAPs have moderate surface area (SABET up to 772 m2 g–1) but demonstrate rather high CO2 uptake (up to 150 mg g–1). Azo functional group is reportedly N2-phobic and hence porous organic polymers (POPs) with azo (−N═N−) units show high CO2/N2 selectivity. TAPs register CO2/N2 selectivity (273 K) that is higher than most azo-POPs reported until date. This favorable property of TAPs is attributed to the simultaneous coexistence of triptycenes (aromatic and three-dimensional rigid with high internal free volume), phenolic-OH (polar and CO2-philic), and azo (CO2-philic and N2-phobic) functional groups in the polymeric framework.

KeyWords AITranslate

triptycene phenolicOH azo units porous organic polymers CO2 uptake CO2/N2 selectivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00264

Chinese Library Classification Number:

Citation Information:

The well-known azo coupling reaction was utilized to yield a new group of triptycene-derived azo polymers (TAPs) bearing phloroglucinol units. TAPs have hierarchical porosity (presence of micropores and mesopores) and are thermally stable. TAPs have moderate surface area (SABET up to 772 m2 g–1) but demonstrate rather high CO2 uptake (up to 150 mg g–1). Azo functional group is reportedly N2-phobic and hence porous organic polymers (POPs) with azo (−N═N−) units show high CO2/N2 selectivity. TAPs register CO2/N2 selectivity (273 K) that is higher than most azo-POPs reported until date. This favorable property of TAPs is attributed to the simultaneous coexistence of triptycenes (aromatic and three-dimensional rigid with high internal free volume), phenolic-OH (polar and CO2-philic), and azo (CO2-philic and N2-phobic) functional groups in the polymeric framework.

quote

GB/T 7714-2015 [1] Ranajit Bera, Mosim Ansari, Akhtar Alam, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00264.
MLA [1] Ranajit Bera, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00264.
APA [1] Ranajit Bera, Mosim Ansari, Akhtar Alam, & Neeladri Das. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00264
IEEE [1] Ranajit Bera, Mosim Ansari, Akhtar Alam, and Neeladri Das, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00264. keywords: {triptycene;phenolicOH;azo units;porous organic polymers;CO2 uptake;CO2/N2 selectivity}