Blade-Coated Hybrid Perovskite Solar Cells with Efficiency > 17%: An In Situ Investigation AITranslate
Abstract AITranslate
Blade-coating has recently emerged as a scalable fabrication method for hybrid perovskite solar cells, but it currently underperforms spin-coating, yielding a power conversion efficiency (PCE) of ∼15% for CH3NH3PbI3 (MAPbI3). We investigate the solidification of MAPbI3 films in situ during spin/blade-coating using optical and X-ray scattering methods. We find that the coating method and conditions profoundly influence the crystallization process, which proceeds through intermediate crystalline solvates. The polymorphism and composition of the solvates are mediated by the solvent removal rate dictated by the process temperature in blade-coating. Low to intermediate temperatures (25–80 °C) yield solvates with differing compositions and yield poor PCEs (∼5–8%) and a large spread (±2.5%). The intermediate solvates are not observed at elevated temperatures (>100 °C), pointing to direct crystallization of the perovskite from the sol–gel ink. These conditions yield large and compact spherulitic domains of perovskite and improve the PCE to ∼13–15% with a narrower spread (< ± 0.5%), while coating at 150 °C yields 17.5% solar cells by inducing in situ decomposition of a small amount of MAPbI3 into PbI2. The insights into the crystallization pathway highlight the current challenges and future opportunities associated with scaling up hybrid perovskite solar cell manufacturing.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00428
Chinese Library Classification Number:
Citation Information:
Blade-coating has recently emerged as a scalable fabrication method for hybrid perovskite solar cells, but it currently underperforms spin-coating, yielding a power conversion efficiency (PCE) of ∼15% for CH3NH3PbI3 (MAPbI3). We investigate the solidification of MAPbI3 films in situ during spin/blade-coating using optical and X-ray scattering methods. We find that the coating method and conditions profoundly influence the crystallization process, which proceeds through intermediate crystalline solvates. The polymorphism and composition of the solvates are mediated by the solvent removal rate dictated by the process temperature in blade-coating. Low to intermediate temperatures (25–80 °C) yield solvates with differing compositions and yield poor PCEs (∼5–8%) and a large spread (±2.5%). The intermediate solvates are not observed at elevated temperatures (>100 °C), pointing to direct crystallization of the perovskite from the sol–gel ink. These conditions yield large and compact spherulitic domains of perovskite and improve the PCE to ∼13–15% with a narrower spread (< ± 0.5%), while coating at 150 °C yields 17.5% solar cells by inducing in situ decomposition of a small amount of MAPbI3 into PbI2. The insights into the crystallization pathway highlight the current challenges and future opportunities associated with scaling up hybrid perovskite solar cell manufacturing.
quote
| GB/T 7714-2015 | [1] Yufei Zhong, Rahim Munir, Jianbo Li, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00428. |
| MLA | [1] Yufei Zhong, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00428. |
| APA | [1] Yufei Zhong, Rahim Munir, Jianbo Li, MingChun Tang, Muhammad R. Niazi, DetlefM. Smilgies, Kui Zhao, & Aram Amassian. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00428 |
| IEEE | [1] Yufei Zhong, Rahim Munir, Jianbo Li, MingChun Tang, Muhammad R. Niazi, DetlefM. Smilgies, Kui Zhao, and Aram Amassian, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00428. |