Synergistic Effect of Inactive Iron Oxide Core on Active Nickel Phosphide Shell for Significant Enhancement in Oxygen Evolution Reaction Activity AITranslate

Department of Materials Science, Indian Association for the Cultivation of Science;Department of Materials Science, Indian Association for the Cultivation of Science; CSIR-Institute of Minerals and Materials Technology;Department of Materials Science, Indian Association for the Cultivation of Science; CSIR-Institute of Minerals and Materials Technology;Department of Materials Science, Indian Association for the Cultivation of Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A unique core–shell nanostructured oxygen evolution reaction (OER) catalyst composed of an electrochemically inactive crystalline iron oxide core and an active amorphous nickel phosphide shell is presented, and this catalyst results in superior OER activity. Even activators enhancing the activity of the OER catalyst by promoting the redox reactions are reported, but here the exclusive position of iron in the nanostructures indeed boosted the efficiency due to ideal placement. Moreover, these nanostructures are also prepared in a sophisticated mechanistic approach in which selectively one metal is phosphidated and the other is not. Interestingly, in the absence of iron, nickel phosphide crystallized in a different shape, but in the presence of iron, this specifically formed amorphous NixP became more efficient for promoting the OER. Details of the formation of this active catalyst are studied; the electrochemical reactions are investigated, and the OER activity is compared with that of different leading metal phosphides.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.7b01141

Chinese Library Classification Number:

Citation Information:

A unique core–shell nanostructured oxygen evolution reaction (OER) catalyst composed of an electrochemically inactive crystalline iron oxide core and an active amorphous nickel phosphide shell is presented, and this catalyst results in superior OER activity. Even activators enhancing the activity of the OER catalyst by promoting the redox reactions are reported, but here the exclusive position of iron in the nanostructures indeed boosted the efficiency due to ideal placement. Moreover, these nanostructures are also prepared in a sophisticated mechanistic approach in which selectively one metal is phosphidated and the other is not. Interestingly, in the absence of iron, nickel phosphide crystallized in a different shape, but in the presence of iron, this specifically formed amorphous NixP became more efficient for promoting the OER. Details of the formation of this active catalyst are studied; the electrochemical reactions are investigated, and the OER activity is compared with that of different leading metal phosphides.

quote

GB/T 7714-2015 [1] Anirban Dutta, Sankararao Mutyala, Aneeya K. Samantara, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.7b01141.
MLA [1] Anirban Dutta, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.7b01141.
APA [1] Anirban Dutta, Sankararao Mutyala, Aneeya K. Samantara, Suman Bera, Bikash Kumar Jena, & Narayan Pradhan. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.7b01141
IEEE [1] Anirban Dutta, Sankararao Mutyala, Aneeya K. Samantara, Suman Bera, Bikash Kumar Jena, and Narayan Pradhan, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.7b01141.