daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Poloxamer Pre-solvation Sheath Ion Encapsulation Strategy for Zinc Anode–Electrolyte Interfaces AITranslate

City University of Hong Kong; Sungkyunkwan University (SKKU); Wuhan University of Technology; City University of Hong Kong; City University of Hong Kong; City University of Hong Kong; Sungkyunkwan University (SKKU); City University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Aqueous metal-ion batteries are considered next-generation energy storage devices with improved safety. However, they suffer from sluggish kinetics and side reactions. This work presents a zinc-ion encapsulation strategy based on the poloxamer pre-solvation sheath for the realization of efficient zinc anode–electrolyte interfaces. The poloxamers can reversibly self-assemble into a pre-solvation sheath by electron-donating effect and effectively shield the ions from the surrounding water. This also lowers the activation energy of desolvation, endowing promoted transference and reaction kinetics. Accordingly, the Zn||Zn cell with the poloxamer electrolyte (Polo-ZnSO4) achieved over 2000 h cycles at 5 mA cm–2 and even over 500 h cycles at 10 mA cm–2. The Zn||MnO2 battery delivers a high and stable capacity of 240.9 mAh g–1 after 1000 cycles at 1 A g–1. This work paves the way for use of encapsulation chemistry for advanced aqueous metal batteries with high Coulombic efficiency and long lifetime.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c02337

Chinese Library Classification Number:

Citation Information:

Aqueous metal-ion batteries are considered next-generation energy storage devices with improved safety. However, they suffer from sluggish kinetics and side reactions. This work presents a zinc-ion encapsulation strategy based on the poloxamer pre-solvation sheath for the realization of efficient zinc anode–electrolyte interfaces. The poloxamers can reversibly self-assemble into a pre-solvation sheath by electron-donating effect and effectively shield the ions from the surrounding water. This also lowers the activation energy of desolvation, endowing promoted transference and reaction kinetics. Accordingly, the Zn||Zn cell with the poloxamer electrolyte (Polo-ZnSO4) achieved over 2000 h cycles at 5 mA cm–2 and even over 500 h cycles at 10 mA cm–2. The Zn||MnO2 battery delivers a high and stable capacity of 240.9 mAh g–1 after 1000 cycles at 1 A g–1. This work paves the way for use of encapsulation chemistry for advanced aqueous metal batteries with high Coulombic efficiency and long lifetime.

quote

GB/T 7714-2015 [1] Kai Yang, Hao Fu, Yixue Duan, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02337.
MLA [1] Kai Yang, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02337.
APA [1] Kai Yang, Hao Fu, Yixue Duan, Zhihao Ma, Dong Wang, Bolong Li, Ho Seok Park, & Derek Ho. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02337
IEEE [1] Kai Yang, Hao Fu, Yixue Duan, Zhihao Ma, Dong Wang, Bolong Li, Ho Seok Park, and Derek Ho, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02337.