Transient Sub-Band-Gap States at Grain Boundaries of CH3NH3PbI3 Perovskite Act as Fast Temperature Relaxation Centers AITranslate
Abstract AITranslate
Extensive spectroscopic studies have been performed on grain boundaries (GBs) of thin-film metal halide perovskites, which inevitably form with current fabrication methods, but direct, on-site determination of the transition energy and dynamics of the associated defect states and their impact on local carrier behaviors have remained elusive. Here, scanning electron microscopy (SEM) correlated to transient absorption microscopy (TAM) on CH3NH3PbI3 perovskite particles is used to identify a defect state ∼60 meV into the band gap at GBs, which accelerates carrier cooling and act as additional energy acceptors. An in-depth statistical analysis performed on a large data set (806 distinct spatial locations) reveals that the shallow defect state, generally considered to be benign, plays a significant role in accelerating carrier cooling, which is detrimental to hot carrier solar cells.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00885
Chinese Library Classification Number:
Citation Information:
Extensive spectroscopic studies have been performed on grain boundaries (GBs) of thin-film metal halide perovskites, which inevitably form with current fabrication methods, but direct, on-site determination of the transition energy and dynamics of the associated defect states and their impact on local carrier behaviors have remained elusive. Here, scanning electron microscopy (SEM) correlated to transient absorption microscopy (TAM) on CH3NH3PbI3 perovskite particles is used to identify a defect state ∼60 meV into the band gap at GBs, which accelerates carrier cooling and act as additional energy acceptors. An in-depth statistical analysis performed on a large data set (806 distinct spatial locations) reveals that the shallow defect state, generally considered to be benign, plays a significant role in accelerating carrier cooling, which is detrimental to hot carrier solar cells.
quote
| GB/T 7714-2015 | [1] Xinyi Jiang, Justin Hoffman, Costas C. Stoumpos, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00885. |
| MLA | [1] Xinyi Jiang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00885. |
| APA | [1] Xinyi Jiang, Justin Hoffman, Costas C. Stoumpos, Mercouri G. Kanatzidis, & Elad Harel. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00885 |
| IEEE | [1] Xinyi Jiang, Justin Hoffman, Costas C. Stoumpos, Mercouri G. Kanatzidis, and Elad Harel, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00885. |