daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Atomically Dispersed Iron–Nitrogen Active Sites within Porphyrinic Triazine-Based Frameworks for Oxygen Reduction Reaction in Both Alkaline and Acidic Media AITranslate

China|University of the Chinese Academy of Sciences; China|University of the Chinese Academy of Sciences; Fujian Institute of Research on the Structure of Matter; Fujian Institute of Research on the Structure of Matter; Tianjin University of Technology; Tianjin University of Technology; Shanghai Institute of Applied Physics; Fujian Institute of Research on the Structure of Matter; China|University of the Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The rational design of highly efficient, low-cost, and durable electrocatalysts to replace platinum-based electrodes for oxygen reduction reaction (ORR) is highly desirable. Although atomically dispersed supported metal catalysts often exhibit excellent catalytic performance with maximized atom efficiency, the fabrication of single-atom catalysts remains a great challenge because of their easy aggregation. Herein, a simple ionothermal method was developed to fabricate atomically dispersed Fe–Nx species on porous porphyrinic triazine-based frameworks (FeSAs/PTF) with high Fe loading up to 8.3 wt %, resulting in highly reactive and stable single-atom ORR catalysts for the first time. Owing to the high density of single-atom Fe–N4 active sites, highly hierarchical porosity, and good conductivity, the as-prepared catalyst FeSAs/PTF-600 exhibited highly efficient activity, methanol tolerance, and superstability for oxygen reduction reaction (ORR) under both alkaline and acidic conditions. This work will bring new inspiration to the design of highly efficient noble-metal-free catalysts at the atomic scale for energy conversion.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00245

Chinese Library Classification Number:

Citation Information:

The rational design of highly efficient, low-cost, and durable electrocatalysts to replace platinum-based electrodes for oxygen reduction reaction (ORR) is highly desirable. Although atomically dispersed supported metal catalysts often exhibit excellent catalytic performance with maximized atom efficiency, the fabrication of single-atom catalysts remains a great challenge because of their easy aggregation. Herein, a simple ionothermal method was developed to fabricate atomically dispersed Fe–Nx species on porous porphyrinic triazine-based frameworks (FeSAs/PTF) with high Fe loading up to 8.3 wt %, resulting in highly reactive and stable single-atom ORR catalysts for the first time. Owing to the high density of single-atom Fe–N4 active sites, highly hierarchical porosity, and good conductivity, the as-prepared catalyst FeSAs/PTF-600 exhibited highly efficient activity, methanol tolerance, and superstability for oxygen reduction reaction (ORR) under both alkaline and acidic conditions. This work will bring new inspiration to the design of highly efficient noble-metal-free catalysts at the atomic scale for energy conversion.

quote

GB/T 7714-2015 [1] JunDong Yi, Rui Xu, Qiao Wu, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00245.
MLA [1] JunDong Yi, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00245.
APA [1] JunDong Yi, Rui Xu, Qiao Wu, Teng Zhang, KeTao Zang, Jun Luo, YuLin Liang, YuanBiao Huang, & Rong Cao. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00245
IEEE [1] JunDong Yi, Rui Xu, Qiao Wu, Teng Zhang, KeTao Zang, Jun Luo, YuLin Liang, YuanBiao Huang, and Rong Cao, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00245.