Abstract AITranslate
Food packaging is critical since proper packaging can extend the shelf life of foods. Currently, petroleum-based plastics, such as poly(ethylene terephthalate) (PET), polyethylene (PE), and polypropylene (PP), are commonly used as packaging materials, but they have led to a lot of waste and environmental pollution. In this study, a previously reported method was modified to fabricate a cellulose nanofiber (CNF) and carboxymethyl cellulose (CMC) paste to make it more homogeneous and less labor-consuming, and it was utilized it as a coating material for molded pulp (MP) food trays. A smooth and uniform dry CNF/CMC coating with a thickness of ∼200 μm was achieved via over-molding. To improve adhesion, chitosan was coated on the MP between layers. Uniaxial tension, “crush strength” compression, and “cross-hatch” and lap-shear adhesion tests were performed to characterize the mechanical enhancement by the coating. Gurley air porosity and water vapor transmission rate tests were conducted to compare the barrier properties against air and moisture between the CNF/CMC-coated MP trays and the uncoated MP trays. Oil and grease resistance testing using the TAPPI-T559 standard showed that coated samples can resist grease much better than uncoated samples. Finally, the trays were lidded with two different kinds of plastic films: poly(lactic acid) (PLA) and poly(ethylene terephthalate) (PET). Raspberries, blueberries, and cherry tomatoes were then used for food storage testing, where it was found that the coating helps extend the shelf life of fruits.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00979
Chinese Library Classification Number:
Citation Information:
Food packaging is critical since proper packaging can extend the shelf life of foods. Currently, petroleum-based plastics, such as poly(ethylene terephthalate) (PET), polyethylene (PE), and polypropylene (PP), are commonly used as packaging materials, but they have led to a lot of waste and environmental pollution. In this study, a previously reported method was modified to fabricate a cellulose nanofiber (CNF) and carboxymethyl cellulose (CMC) paste to make it more homogeneous and less labor-consuming, and it was utilized it as a coating material for molded pulp (MP) food trays. A smooth and uniform dry CNF/CMC coating with a thickness of ∼200 μm was achieved via over-molding. To improve adhesion, chitosan was coated on the MP between layers. Uniaxial tension, “crush strength” compression, and “cross-hatch” and lap-shear adhesion tests were performed to characterize the mechanical enhancement by the coating. Gurley air porosity and water vapor transmission rate tests were conducted to compare the barrier properties against air and moisture between the CNF/CMC-coated MP trays and the uncoated MP trays. Oil and grease resistance testing using the TAPPI-T559 standard showed that coated samples can resist grease much better than uncoated samples. Finally, the trays were lidded with two different kinds of plastic films: poly(lactic acid) (PLA) and poly(ethylene terephthalate) (PET). Raspberries, blueberries, and cherry tomatoes were then used for food storage testing, where it was found that the coating helps extend the shelf life of fruits.
quote
| GB/T 7714-2015 | [1] Jingxuan Zhang, Jeffrey P. Youngblood. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00979. |
| MLA | [1] Jingxuan Zhang, and Jeffrey P. Youngblood. ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00979. |
| APA | [1] Jingxuan Zhang, & Jeffrey P. Youngblood. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00979 |
| IEEE | [1] Jingxuan Zhang and Jeffrey P. Youngblood, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00979. keywords: {food packaging;cellulose nanofibrils;carboxymethyl cellulose;mechanical strength enhancer;barrier properties} |