Conformational Energy Settled Crystallization Behaviors of Poly(l-lactic acid) AITranslate
Abstract AITranslate
Polymer crystallization is crucial to the properties of polymers, which are determined by thermal dynamics and kinetics. The formation of polymorphism has turned out to be very important for applications of poly(l-lactic acid) (PLLA), because it has evolved into a competitive commodity material over the past decade. In the in situ wide-angle X-ray scattering study, it shows the growth of α-crystal of thermally treated PLLA at Tc = 80 and 90 °C, which was considered only appropriate for the crystallization of its δ-form. A part of α-embryos and the locally ordered structures developed for the α-crystal may adjust their chain conformations from getting adapted to the crystallization of the δ-crystal, while the others continue to grow in their own α-form. Two crystal forms crystallize on different dynamic pathways, and the δ-form should be an independent crystal, better identified as the “δ-” instead of the previous “α′-”.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00722
Chinese Library Classification Number:
Citation Information:
Polymer crystallization is crucial to the properties of polymers, which are determined by thermal dynamics and kinetics. The formation of polymorphism has turned out to be very important for applications of poly(l-lactic acid) (PLLA), because it has evolved into a competitive commodity material over the past decade. In the in situ wide-angle X-ray scattering study, it shows the growth of α-crystal of thermally treated PLLA at Tc = 80 and 90 °C, which was considered only appropriate for the crystallization of its δ-form. A part of α-embryos and the locally ordered structures developed for the α-crystal may adjust their chain conformations from getting adapted to the crystallization of the δ-crystal, while the others continue to grow in their own α-form. Two crystal forms crystallize on different dynamic pathways, and the δ-form should be an independent crystal, better identified as the “δ-” instead of the previous “α′-”.
quote
| GB/T 7714-2015 | [1] Cunliang Hu, Tongxin Lv, Jingqing Li, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00722. |
| MLA | [1] Cunliang Hu, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00722. |
| APA | [1] Cunliang Hu, Tongxin Lv, Jingqing Li, Shaoyong Huang, Hongfei Li, Jizhong Chen, Donghong Yu, Jesper de Claville Christiansen, Shichun Jiang, & Lijia An. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00722 |
| IEEE | [1] Cunliang Hu, Tongxin Lv, Jingqing Li, Shaoyong Huang, Hongfei Li, Jizhong Chen, Donghong Yu, Jesper de Claville Christiansen, Shichun Jiang, and Lijia An, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00722. keywords: {δ and αcrystal;dynamic pathways;independent crystal;in situ wideangle Xray scattering;polymorphism;poly(llactic acid)} |