daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hole-Transporting Self-Assembled Monolayer Enables Efficient Single-Crystal Perovskite Solar Cells with Enhanced Stability AITranslate

King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); The Hong Kong Polytechnic University; King Abdullah University of Science and Technology (KAUST);Saudi Aramco Research & Development Center, Dhahran 31311;Saudi Aramco Research & Development Center, Dhahran 31311;Saudi Aramco Research & Development Center, Dhahran 31311; King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The difficulty of growing perovskite single crystals in configurations suitable for efficient photovoltaic devices has hampered their exploration as solar cell materials, despite their potential to advance perovskite photovoltaic technology beyond polycrystalline films through markedly lower defect densities and desirable optoelectronic properties. While polycrystalline film absorbers can be deposited on myriad substrates, perovskite single crystals fit for high-efficiency devices have only been demonstrated on hydrophobic hole-transport layers [HTLs, e.g., poly(triaryl amine) (PTAA)], which has severely restricted the avenues for enhancing device efficiency and stability. Herein, we report the growth of mixed-cation FA0.6MA0.4PbI3 perovskite single crystals on a hydrophilic self-assembled monolayer {SAM, [2-(3,6-dimethoxy-9H-carbazol-9-yl)ethyl]phosphonic acid), (MeO-2PACz)} HTL surface. Compared with PTAA, the MeO-2PACz SAM promotes the mechanical adhesion of the perovskite on the substrate, enabling the fabrication of inverted solar cells with substantially enhanced operational stability and power conversion efficiencies of up to 23.1%, setting a new benchmark for single-crystal perovskite solar cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02333

Chinese Library Classification Number:

Citation Information:

The difficulty of growing perovskite single crystals in configurations suitable for efficient photovoltaic devices has hampered their exploration as solar cell materials, despite their potential to advance perovskite photovoltaic technology beyond polycrystalline films through markedly lower defect densities and desirable optoelectronic properties. While polycrystalline film absorbers can be deposited on myriad substrates, perovskite single crystals fit for high-efficiency devices have only been demonstrated on hydrophobic hole-transport layers [HTLs, e.g., poly(triaryl amine) (PTAA)], which has severely restricted the avenues for enhancing device efficiency and stability. Herein, we report the growth of mixed-cation FA0.6MA0.4PbI3 perovskite single crystals on a hydrophilic self-assembled monolayer {SAM, [2-(3,6-dimethoxy-9H-carbazol-9-yl)ethyl]phosphonic acid), (MeO-2PACz)} HTL surface. Compared with PTAA, the MeO-2PACz SAM promotes the mechanical adhesion of the perovskite on the substrate, enabling the fabrication of inverted solar cells with substantially enhanced operational stability and power conversion efficiencies of up to 23.1%, setting a new benchmark for single-crystal perovskite solar cells.

quote

GB/T 7714-2015 [1] Khulud Almasabi, Xiaopeng Zheng, Bekir Turedi, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02333.
MLA [1] Khulud Almasabi, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02333.
APA [1] Khulud Almasabi, Xiaopeng Zheng, Bekir Turedi, Abdullah Y. Alsalloum, Muhammad Naufal Lintangpradipto, Jun Yin, Luis GutiérrezArzaluz, Konstantinos Kotsovos, Aqil Jamal, Issam Gereige, Omar F. Mohammed, & Osman M. Bakr. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02333
IEEE [1] Khulud Almasabi, Xiaopeng Zheng, Bekir Turedi, Abdullah Y. Alsalloum, Muhammad Naufal Lintangpradipto, Jun Yin, Luis GutiérrezArzaluz, Konstantinos Kotsovos, Aqil Jamal, Issam Gereige, Omar F. Mohammed, and Osman M. Bakr, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02333.