Binding Studies of Cationic Conjugated Polymers and DNA for Label-Free Fluorescent Biosensors AITranslate
Abstract AITranslate
Cationic conjugated polymers (CCPs), especially polythiophene, have been extensively used as probes for developing DNA and aptamer-based biosensors. Although many interesting applications have been achieved, a fundamental understanding of this system remains quite limited. In this work, we performed systematic binding assays to understand the interactions between poly(3-(3′-N,N,N-triethylamino-1′-propyloxy)-4-methyl-2,5-thiophene) (PMNT) and DNA. The fluorescence of PMNT at 530 nm initially decreased and then a peak at 580 nm emerged after binding with single-stranded DNA (ssDNA). The binding force between PMNT and DNA was dominated by electrostatic interactions at first and then DNA base-mediated interactions also became important. Since the bases in double-stranded DNA (dsDNA) were shielded, their fluorescence changes were quite different. To best differentiate ssDNA and dsDNA, the optimal pH was between 6 and 8, and the optimal NaCl concentration was around 0.3 M. Moreover, by changing the sequence and length of ssDNA, poly-T had the largest fluorescence shift and poly-A had the smallest change. Under the optimized conditions, the PMNT-based biosensor had a detection limit of 1 nM DNA, which was similar to the SYBR Green I-based assay.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c00986
Chinese Library Classification Number:
Citation Information:
Cationic conjugated polymers (CCPs), especially polythiophene, have been extensively used as probes for developing DNA and aptamer-based biosensors. Although many interesting applications have been achieved, a fundamental understanding of this system remains quite limited. In this work, we performed systematic binding assays to understand the interactions between poly(3-(3′-N,N,N-triethylamino-1′-propyloxy)-4-methyl-2,5-thiophene) (PMNT) and DNA. The fluorescence of PMNT at 530 nm initially decreased and then a peak at 580 nm emerged after binding with single-stranded DNA (ssDNA). The binding force between PMNT and DNA was dominated by electrostatic interactions at first and then DNA base-mediated interactions also became important. Since the bases in double-stranded DNA (dsDNA) were shielded, their fluorescence changes were quite different. To best differentiate ssDNA and dsDNA, the optimal pH was between 6 and 8, and the optimal NaCl concentration was around 0.3 M. Moreover, by changing the sequence and length of ssDNA, poly-T had the largest fluorescence shift and poly-A had the smallest change. Under the optimized conditions, the PMNT-based biosensor had a detection limit of 1 nM DNA, which was similar to the SYBR Green I-based assay.
quote
| GB/T 7714-2015 | [1] Pengbo Zhang, Chang Lu, Chenqi Niu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00986. |
| MLA | [1] Pengbo Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00986. |
| APA | [1] Pengbo Zhang, Chang Lu, Chenqi Niu, Xiaoyu Wang, Zhengping Li, & Juewen Liu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00986 |
| IEEE | [1] Pengbo Zhang, Chang Lu, Chenqi Niu, Xiaoyu Wang, Zhengping Li, and Juewen Liu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00986. keywords: {cationic conjugated polymers;DNA detection;biosensors;aptamers;fluorescence} |