Ionic Functionalized Magnetic Porous Polymers as Advanced Materials for High-Efficiency Water Decontamination: Bactericidal and Iodine Adsorption AITranslate

Weifang Medical University;Sunshine Union Hospital, Weifang 261072; Weifang Medical University; Weifang Medical University; Weifang Medical University; Weifang Medical University; Weifang Medical University; Weifang Medical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The relentless exploration of environmentally friendly remediation materials for high-efficiency killing of bacteria and capture of radioactive iodine from water is an eternal mutual topic among both academia and industry. Herein, a magnetic ionic porous organic polymer (iFP-POP) featuring sustainable and recyclable capacity was prepared via the “multivariate” strategy combined with subsequent postsynthesis modification and served as an advanced material to purify polluted water. The iFP-POP with an ultrafine magnetic γ-Fe2O3 core and a hierarchical porous polymer layer was prepared via a facile and scalable synthesis strategy, in which γ-Fe2O3 was formed directly during the coupling reaction. The iFP-POP featured abundant binding sites for I2, including highly polar heteroatoms, quaternary ammonium ionic groups, magnetic γ-Fe2O3, and electronegative cyclopentadiene, simultaneously, and presented ultrahigh I2 capture capacities. Notably, iFP-POP recovered easily and rapidly from various solutions by using a magnet, which could be easily regenerated with almost no performance degradation. The unique structure endowed prominent antimicrobial activity to iFP-POP to act as a broad-spectrum bactericide. In vitro assay demonstrated that iFP-POP displays a cation-enhanced photothermal antibacterial effect toward both Gram-positive Staphylococcus aureus (99.93%) and Gram-negative Escherichia coli (94.99%). Furthermore, the encapsulation of I2 endowed iFP-POP with the diffusion antibacterial effect, allowing iFP-POP to act as a recyclable antibacterial material. This work proposes inspiring information for the rational design and controllable fabrication of targeted POP-based materials for environmental pollution management.

KeyWords AITranslate

magnetic porous organic polymer quaternary ammonium salt water purification antibacterial iodine capture
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01811

Chinese Library Classification Number:

Citation Information:

The relentless exploration of environmentally friendly remediation materials for high-efficiency killing of bacteria and capture of radioactive iodine from water is an eternal mutual topic among both academia and industry. Herein, a magnetic ionic porous organic polymer (iFP-POP) featuring sustainable and recyclable capacity was prepared via the “multivariate” strategy combined with subsequent postsynthesis modification and served as an advanced material to purify polluted water. The iFP-POP with an ultrafine magnetic γ-Fe2O3 core and a hierarchical porous polymer layer was prepared via a facile and scalable synthesis strategy, in which γ-Fe2O3 was formed directly during the coupling reaction. The iFP-POP featured abundant binding sites for I2, including highly polar heteroatoms, quaternary ammonium ionic groups, magnetic γ-Fe2O3, and electronegative cyclopentadiene, simultaneously, and presented ultrahigh I2 capture capacities. Notably, iFP-POP recovered easily and rapidly from various solutions by using a magnet, which could be easily regenerated with almost no performance degradation. The unique structure endowed prominent antimicrobial activity to iFP-POP to act as a broad-spectrum bactericide. In vitro assay demonstrated that iFP-POP displays a cation-enhanced photothermal antibacterial effect toward both Gram-positive Staphylococcus aureus (99.93%) and Gram-negative Escherichia coli (94.99%). Furthermore, the encapsulation of I2 endowed iFP-POP with the diffusion antibacterial effect, allowing iFP-POP to act as a recyclable antibacterial material. This work proposes inspiring information for the rational design and controllable fabrication of targeted POP-based materials for environmental pollution management.

quote

GB/T 7714-2015 [1] Changqing Miao, Nailing Tang, Lin Shi, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01811.
MLA [1] Changqing Miao, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01811.
APA [1] Changqing Miao, Nailing Tang, Lin Shi, Shaoyu Wang, Pengpeng Ji, Jian Zhang, Zengyao Wang, & Baolong Zhou. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01811
IEEE [1] Changqing Miao, Nailing Tang, Lin Shi, Shaoyu Wang, Pengpeng Ji, Jian Zhang, Zengyao Wang, and Baolong Zhou, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01811. keywords: {magnetic porous organic polymer;quaternary ammonium salt;water purification;antibacterial;iodine capture}