Electroactive and Conformal Coatings of Oxidative Chemical Vapor Deposition Polymers for Oxygen Electroreduction AITranslate

University of Nebraska−Lincoln; University of Nebraska−Lincoln; University of Nebraska−Lincoln; University of Nebraska−Lincoln
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polymer from 3,4-ethylenedioxythiophene (EDOT) was synthesized using oxidative chemical vapor deposition (oCVD). To enable the synthesis of PEDOT, two different oxidants, antimony pentachloride (SbCl5) and vanadium oxytrichloride (VOCl3), were utilized. The effect of deposition temperature on the polymer electroactivity and conductivity was evaluated by measuring the overpotential for the oxygen reduction reaction and film electrical conductivity, respectively. PEDOT films with conductivity values of ∼2000 S/cm were deposited in a single step coating and doping process. X-ray photoelectron spectroscopy revealed that the residual metalloid within polymer films, in the case of SbCl5, is contributing to the hole conductivity. The electrocatalytic activity of deposited material in oxygen reduction reaction (ORR) was studied; the results indicate a direct relationship between the conductivity values and the electrocatalytic activities of the deposited films. The unique potential offered by oCVD to coat PEDOT conformally enabled us to apply a coat of electroactive polymers on complex structures of a gas diffusion layer fabric, carbon cloth. Using our approach, we imparted stable electrocatalytic activity to carbon cloth electrodes and fabricated all-organic electrodes for ORR.

KeyWords AITranslate

oxidative chemical vapor deposition (oCVD) poly(3 4ethylenedioxythiophene) (PEDOT) oxygen reduction reaction (ORR) highly Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00240

Chinese Library Classification Number:

Citation Information:

Polymer from 3,4-ethylenedioxythiophene (EDOT) was synthesized using oxidative chemical vapor deposition (oCVD). To enable the synthesis of PEDOT, two different oxidants, antimony pentachloride (SbCl5) and vanadium oxytrichloride (VOCl3), were utilized. The effect of deposition temperature on the polymer electroactivity and conductivity was evaluated by measuring the overpotential for the oxygen reduction reaction and film electrical conductivity, respectively. PEDOT films with conductivity values of ∼2000 S/cm were deposited in a single step coating and doping process. X-ray photoelectron spectroscopy revealed that the residual metalloid within polymer films, in the case of SbCl5, is contributing to the hole conductivity. The electrocatalytic activity of deposited material in oxygen reduction reaction (ORR) was studied; the results indicate a direct relationship between the conductivity values and the electrocatalytic activities of the deposited films. The unique potential offered by oCVD to coat PEDOT conformally enabled us to apply a coat of electroactive polymers on complex structures of a gas diffusion layer fabric, carbon cloth. Using our approach, we imparted stable electrocatalytic activity to carbon cloth electrodes and fabricated all-organic electrodes for ORR.

quote

GB/T 7714-2015 [1] Shayan Kaviani, Mahdi Mohammadi Ghaleni, Elham Tavakoli, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00240.
MLA [1] Shayan Kaviani, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00240.
APA [1] Shayan Kaviani, Mahdi Mohammadi Ghaleni, Elham Tavakoli, & Siamak Nejati. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00240
IEEE [1] Shayan Kaviani, Mahdi Mohammadi Ghaleni, Elham Tavakoli, and Siamak Nejati, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00240. keywords: {oxidative chemical vapor deposition (oCVD);poly(3;4ethylenedioxythiophene) (PEDOT);oxygen reduction reaction (ORR);highly;Show More}