daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Thermodynamic modeling of the Sn–V binary system AITranslate

Central South University; China University of Geosciences; General Research Institute for Nonferrous Metals; General Research Institute for Nonferrous Metals
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The Sn–V binary system was thermodynamically modeled using the CALPHAD approach combined with first-principles calculations. The predicted Gibbs free energy of the end-members in sublattice models of “ V 3Sn” phase by the first-principles calculations was used to describe the lattice stabilities. A set of thermodynamic parameters for the Sn–V system was obtained using the PanOptimizer program in Pandat software. The calculated phase diagram and thermodynamic properties agree well with the reported experimental data.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2009.03.003

Chinese Library Classification Number:

Citation Information:

The Sn–V binary system was thermodynamically modeled using the CALPHAD approach combined with first-principles calculations. The predicted Gibbs free energy of the end-members in sublattice models of “ V 3Sn” phase by the first-principles calculations was used to describe the lattice stabilities. A set of thermodynamic parameters for the Sn–V system was obtained using the PanOptimizer program in Pandat software. The calculated phase diagram and thermodynamic properties agree well with the reported experimental data.

quote

GB/T 7714-2015 [1] Q. Yue, Y.Q. Liu, M.Y. Chu, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.03.003.
MLA [1] Q. Yue, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.03.003.
APA [1] Q. Yue, Y.Q. Liu, M.Y. Chu, & J.Y. Shen. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.03.003
IEEE [1] Q. Yue, Y.Q. Liu, M.Y. Chu, and J.Y. Shen, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2009.03.003.