Interdiffusion behaviors and mechanical properties in Zr-Nb-Hf system AITranslate
Abstract AITranslate
The diffusion behavior and mechanical properties of the Zr-Nb-Hf system were analyzed using diffusion couple technology and nanoindentation techniques. The diffusion couples were annealed at 1523 K for 24 h, and the compositional profile of the diffusion region was determined using electron probe microanalysis. The main diffusion coefficients, cross-diffusion coefficients, and impurity diffusion coefficients were calculated using the Whittle and Green method, as well as the generalized Hall method. Furthermore, the hardness and Young`s modulus of the alloy with different compositions were calculated by Oliver method, based on load-displacement curves obtained from nanoindentation tests. Additionally, the wear resistance and resistance to plastic deformation of the Zr-Nb-Hf alloys were inferred. These results contribute to the existing database of diffusion kinetics and mechanical properties in the Zr-Nb-Hf system, providing valuable references for the development of Zr-Nb-Hf-based alloys with exceptional properties.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2023.102634
Chinese Library Classification Number:
Citation Information:
The diffusion behavior and mechanical properties of the Zr-Nb-Hf system were analyzed using diffusion couple technology and nanoindentation techniques. The diffusion couples were annealed at 1523 K for 24 h, and the compositional profile of the diffusion region was determined using electron probe microanalysis. The main diffusion coefficients, cross-diffusion coefficients, and impurity diffusion coefficients were calculated using the Whittle and Green method, as well as the generalized Hall method. Furthermore, the hardness and Young`s modulus of the alloy with different compositions were calculated by Oliver method, based on load-displacement curves obtained from nanoindentation tests. Additionally, the wear resistance and resistance to plastic deformation of the Zr-Nb-Hf alloys were inferred. These results contribute to the existing database of diffusion kinetics and mechanical properties in the Zr-Nb-Hf system, providing valuable references for the development of Zr-Nb-Hf-based alloys with exceptional properties.
quote
| GB/T 7714-2015 | [1] Liyang Fang, Jun Wang, Chenran Xu, et al. Calphad, 2023(83). DOI:10.1016/j.calphad.2023.102634. |
| MLA | [1] Liyang Fang, et al., Calphad, no. 83, 2023, https://doi.org/10.1016/j.calphad.2023.102634. |
| APA | [1] Liyang Fang, Jun Wang, Chenran Xu, Xiancong He, Guanglong Xu, Xiaoma Tao, Yifang Ouyang, & Yong Du. (2023). Calphad(83). https://doi.org/10.1016/j.calphad.2023.102634 |
| IEEE | [1] Liyang Fang, Jun Wang, Chenran Xu, Xiancong He, Guanglong Xu, Xiaoma Tao, Yifang Ouyang, and Yong Du, Calphad, no. 83, 2023, doi: 10.1016/j.calphad.2023.102634. |