Recent Advances in Physical Sensors Based on Electrospinning Technology AITranslate
Abstract AITranslate
In the past decades, the rapid development of the Internet of Things (IoT) technology and artificial intelligence (AI) has driven the research boom of physical sensors. Material selection, structure design, and performance research for physical sensors have attracted extensive attention from worldwide researchers in the field of advanced manufacturing. Significant technological progress has been made in the area of physical sensors for applications in various fields such as electronic skin, biomedicine, and tissue engineering. There are many methods (e.g., electrospinning, screen printing, or rotary coating) to prepare physical sensors. Among them, nanofibers or nanofiber membranes prepared by electrospinning have the advantages of a nanosize effect, high specific surface area, and high porosity over other reported materials used for physical sensors. In this review, the working principles of various physical sensors including pressure sensors, strain sensors, temperature sensors, and humidity sensors are first introduced; recent research progress of electrospun nanofiber-based physical sensors is then summarized. Finally, future research trends and associated challenges of large-scale adoption of electrospun physical sensors are proposed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.3c00144
Chinese Library Classification Number:
Citation Information:
In the past decades, the rapid development of the Internet of Things (IoT) technology and artificial intelligence (AI) has driven the research boom of physical sensors. Material selection, structure design, and performance research for physical sensors have attracted extensive attention from worldwide researchers in the field of advanced manufacturing. Significant technological progress has been made in the area of physical sensors for applications in various fields such as electronic skin, biomedicine, and tissue engineering. There are many methods (e.g., electrospinning, screen printing, or rotary coating) to prepare physical sensors. Among them, nanofibers or nanofiber membranes prepared by electrospinning have the advantages of a nanosize effect, high specific surface area, and high porosity over other reported materials used for physical sensors. In this review, the working principles of various physical sensors including pressure sensors, strain sensors, temperature sensors, and humidity sensors are first introduced; recent research progress of electrospun nanofiber-based physical sensors is then summarized. Finally, future research trends and associated challenges of large-scale adoption of electrospun physical sensors are proposed.
quote
| GB/T 7714-2015 | [1] Hanlin Cao, Shanshan Chai, Zifang Tan, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00144. |
| MLA | [1] Hanlin Cao, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00144. |
| APA | [1] Hanlin Cao, Shanshan Chai, Zifang Tan, Hong Wu, Xue Mao, Liang Wei, Fenglei Zhou, Runjun Sun, & Chengkun Liu. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00144 |
| IEEE | [1] Hanlin Cao, Shanshan Chai, Zifang Tan, Hong Wu, Xue Mao, Liang Wei, Fenglei Zhou, Runjun Sun, and Chengkun Liu, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00144. |