High-Efficiency Circularly Polarized Luminescence from Twisted Tetraarylethylene-Bridged Polybissilsesquioxane Nanotubes AITranslate

Soochow University; Soochow University; South China University of Technology; Soochow University; Soochow University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Circularly polarized luminescence (CPL)-active materials have attracted increasing attention due to their applications in chiral sensing and optoelectronics. However, it is still a challenging task to fabricate CPL materials with large luminescence dissymmetry factors and strong emission intensities in the solid state. In this work, two single-handed twisted tetraarylethylene (TAE)-bridged polybissilsesquioxane nanotubes have been facilely constructed through a supramolecular templating polymerization of TAE-bridged bis(triethoxysilane) with aggregation-induced emission properties, using self-assemblies of a pair of chiral amino acid-based cationic amphiphiles as the supramolecular templates. It is found that the chirality has been transferred from the self-assemblies to the polybissilsesquioxane nanotubes. The resulting hybrid silicas show high thermal stabilities and bright CPL with the fluorescence quantum yield up to 62.8%.

KeyWords AITranslate

circularly polarized luminescence tetraarylethylene aggregationinduced emission polybissilsesquioxane supramolecular Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01112

Chinese Library Classification Number:

Citation Information:

Circularly polarized luminescence (CPL)-active materials have attracted increasing attention due to their applications in chiral sensing and optoelectronics. However, it is still a challenging task to fabricate CPL materials with large luminescence dissymmetry factors and strong emission intensities in the solid state. In this work, two single-handed twisted tetraarylethylene (TAE)-bridged polybissilsesquioxane nanotubes have been facilely constructed through a supramolecular templating polymerization of TAE-bridged bis(triethoxysilane) with aggregation-induced emission properties, using self-assemblies of a pair of chiral amino acid-based cationic amphiphiles as the supramolecular templates. It is found that the chirality has been transferred from the self-assemblies to the polybissilsesquioxane nanotubes. The resulting hybrid silicas show high thermal stabilities and bright CPL with the fluorescence quantum yield up to 62.8%.

quote

GB/T 7714-2015 [1] Fengmin Han, Fengyun Shi, Hongkun Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01112.
MLA [1] Fengmin Han, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01112.
APA [1] Fengmin Han, Fengyun Shi, Hongkun Li, Yonggang Yang, & Yongfang Li. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01112
IEEE [1] Fengmin Han, Fengyun Shi, Hongkun Li, Yonggang Yang, and Yongfang Li, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01112. keywords: {circularly polarized luminescence;tetraarylethylene;aggregationinduced emission;polybissilsesquioxane;supramolecular;Show More}