Preparation of High-Performance Polyethylene Composite Materials Reinforced with Cellulose Nanofiber: Simultaneous Nanofibrillation of Wood Pulp Fibers during Melt-Compounding Using Urea and Diblock Copolymer Dispersant AITranslate

Kyoto University; Kyoto University; Kyoto University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Production of nanocomposites from macro-scale materials in situ in a melting compounder is highly desirable yet challenging. In this study, we develop a highly efficient approach for the preparation of cellulose nanofiber (CNF)-reinforced high-density polyethylene (HDPE) composite materials from as-received wood pulp fibers, in which nanofibrillation-assisting plasticizers (urea and urea derivatives) and a diblock copolymer dispersant are used. The most effective plasticizer is urea, which plays a crucial role in producing CNF with less fragmentation during the kneading step, owing to the plasticization/nanofibrillation and the reaction with hydroxyl groups of cellulose fibers into a carbamate. The diblock copolymer as a dispersant enables the stabilization of the appropriate dispersion of the produced CNF in nonpolar HDPE. The resulting composites exhibit significantly improved mechanical properties, including a 6.9-fold increase in the Young’s modulus with 10 wt % loading of wood pulp fibers over that of neat HDPE.

KeyWords AITranslate

cellulose nanofiber urea polymer dispersant nanofibrillation fragmentation dispersion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00071

Chinese Library Classification Number:

Citation Information:

Production of nanocomposites from macro-scale materials in situ in a melting compounder is highly desirable yet challenging. In this study, we develop a highly efficient approach for the preparation of cellulose nanofiber (CNF)-reinforced high-density polyethylene (HDPE) composite materials from as-received wood pulp fibers, in which nanofibrillation-assisting plasticizers (urea and urea derivatives) and a diblock copolymer dispersant are used. The most effective plasticizer is urea, which plays a crucial role in producing CNF with less fragmentation during the kneading step, owing to the plasticization/nanofibrillation and the reaction with hydroxyl groups of cellulose fibers into a carbamate. The diblock copolymer as a dispersant enables the stabilization of the appropriate dispersion of the produced CNF in nonpolar HDPE. The resulting composites exhibit significantly improved mechanical properties, including a 6.9-fold increase in the Young’s modulus with 10 wt % loading of wood pulp fibers over that of neat HDPE.

quote

GB/T 7714-2015 [1] Keita Sakakibara, Yoshihito Moriki, Yoshinobu Tsujii. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00071.
MLA [1] Keita Sakakibara, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00071.
APA [1] Keita Sakakibara, Yoshihito Moriki, & Yoshinobu Tsujii. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00071
IEEE [1] Keita Sakakibara, Yoshihito Moriki, and Yoshinobu Tsujii, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00071. keywords: {cellulose nanofiber;urea;polymer dispersant;nanofibrillation;fragmentation;dispersion}