Improved Sensitivity of Flexible Conductive Composites Throughout the Working Strain Range Based on Bioinspired Strain Redistribution AITranslate

Hubei University of Technology; Hubei University of Technology; Georgia Institute of Technology; Hubei University of Technology; Hubei University of Technology; Hubei University of Technology; Hubei University of Technology; Hubei University of Technology; Georgia Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Elastomer conductive composites (ECCs) are wonderful candidates for stretchable strain sensors. However, the sensitivity of ECC-based flexible strain sensors is limited in low-strain range, the main working range for human movements, due to the insignificant geometric change of the sample shape and weak tunneling effect of the conductive network. Herein, bioinspired heterogeneous thermoplastic polyurethane (TPU)/carbon black (CB) composites (TCs) are assembled by hot pressing two TCs with different Young’s moduli in series. The modulus of the TCs is controlled by the CB content, Young’s modulus of TPU, and plasticizer content. Experimental results and finite element analysis (FEA) confirm that the low Young’s modulus component undergoes higher strain compared with the high Young’s modulus component, resulting in a more serious change of the conductive network and higher gauge factor (GF) values. Compared with homogeneous TCs, the GF of heterogeneous TCs was improved by a factor of 20.7 and 9.6 in the low-strain (0–6%) and high-strain range, respectively. The relationship between modulus variety and GF is quantitatively described, and the GF values depend on the Young’s modulus of the individual components. Constructing a heterogeneous structure with different Young’s moduli is a valuable and facile way to increase the sensitivity of ECC-based flexible strain sensors.

KeyWords AITranslate

heterogeneous composites flexible strain sensor Young’s modulus difference strain redistribution sensitivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01403

Chinese Library Classification Number:

Citation Information:

Elastomer conductive composites (ECCs) are wonderful candidates for stretchable strain sensors. However, the sensitivity of ECC-based flexible strain sensors is limited in low-strain range, the main working range for human movements, due to the insignificant geometric change of the sample shape and weak tunneling effect of the conductive network. Herein, bioinspired heterogeneous thermoplastic polyurethane (TPU)/carbon black (CB) composites (TCs) are assembled by hot pressing two TCs with different Young’s moduli in series. The modulus of the TCs is controlled by the CB content, Young’s modulus of TPU, and plasticizer content. Experimental results and finite element analysis (FEA) confirm that the low Young’s modulus component undergoes higher strain compared with the high Young’s modulus component, resulting in a more serious change of the conductive network and higher gauge factor (GF) values. Compared with homogeneous TCs, the GF of heterogeneous TCs was improved by a factor of 20.7 and 9.6 in the low-strain (0–6%) and high-strain range, respectively. The relationship between modulus variety and GF is quantitatively described, and the GF values depend on the Young’s modulus of the individual components. Constructing a heterogeneous structure with different Young’s moduli is a valuable and facile way to increase the sensitivity of ECC-based flexible strain sensors.

quote

GB/T 7714-2015 [1] Rong Zhang, Hailong Hu, Zhijian Sun, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01403.
MLA [1] Rong Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01403.
APA [1] Rong Zhang, Hailong Hu, Zhijian Sun, Siqi Li, Zhuohang Liu, Shengfei Hu, Xudong Fu, Qingting Liu, & Ching Ping Wong. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01403
IEEE [1] Rong Zhang, Hailong Hu, Zhijian Sun, Siqi Li, Zhuohang Liu, Shengfei Hu, Xudong Fu, Qingting Liu, and Ching Ping Wong, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01403. keywords: {heterogeneous composites;flexible strain sensor;Young’s modulus difference;strain redistribution;sensitivity}