Modeling of efficient charge transfer materials of 4,6-di(thiophen-2-yl)pyrimidine derivatives: Quantum chemical investigations AITranslate

King Khalid University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Efficient charge transfer materials have been designed and investigated. • DFT and TDDFT approaches have been applied. • Improved ICT reduced the energy gap and tuned the properties. • Smaller hole reorganization energy showed materials might be similar to pentacene. The 4,6-di(thiophen-2-yl)pyrimidine has alternate pi-rich and pi-poor units. To reduce the HOMO–LUMO energy gap and improve the intra-molecular charge transfer pi-backbone has been elongated along with push–pull strategy. The ground state geometries have been optimized by using density functional theory. The frontier molecular orbitals, i.e., highest occupied molecular orbitals (HOMOs) and lowest unoccupied molecular orbitals (LUMOs) have been conferred. The absorption spectra have been computed by using time dependent density functional theory. On the basis of ionization potentials, electron affinities and reorganization energies charge transfer properties have been discussed. We tuned the electronic, photophysical and charge transfer properties of 4,6-di(thiophen-2-yl)pyrimidine derivatives. It is expected that new designed derivatives might be better/comparable to commonly used hole transfer material (pentacene). The smaller reorganization energies revealing that the electron transfer properties of new designed derivatives might be better/comparable to commonly used electron transfer materials (tris(8-hydroxyquinolinato)aluminum). The structure–property relationship has been discussed. Graphical abstract Download : Download high-res image (45KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.09.003

Chinese Library Classification Number:

Citation Information:

Highlights • Efficient charge transfer materials have been designed and investigated. • DFT and TDDFT approaches have been applied. • Improved ICT reduced the energy gap and tuned the properties. • Smaller hole reorganization energy showed materials might be similar to pentacene. The 4,6-di(thiophen-2-yl)pyrimidine has alternate pi-rich and pi-poor units. To reduce the HOMO–LUMO energy gap and improve the intra-molecular charge transfer pi-backbone has been elongated along with push–pull strategy. The ground state geometries have been optimized by using density functional theory. The frontier molecular orbitals, i.e., highest occupied molecular orbitals (HOMOs) and lowest unoccupied molecular orbitals (LUMOs) have been conferred. The absorption spectra have been computed by using time dependent density functional theory. On the basis of ionization potentials, electron affinities and reorganization energies charge transfer properties have been discussed. We tuned the electronic, photophysical and charge transfer properties of 4,6-di(thiophen-2-yl)pyrimidine derivatives. It is expected that new designed derivatives might be better/comparable to commonly used hole transfer material (pentacene). The smaller reorganization energies revealing that the electron transfer properties of new designed derivatives might be better/comparable to commonly used electron transfer materials (tris(8-hydroxyquinolinato)aluminum). The structure–property relationship has been discussed. Graphical abstract Download : Download high-res image (45KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Ahmad Irfan. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.09.003.
MLA [1] Ahmad Irfan. Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.09.003.
APA [1] Ahmad Irfan. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.09.003
IEEE [1] Ahmad Irfan, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.09.003.