Nitric oxide release for improving performance of implantable chemical sensors – A review AITranslate
Abstract AITranslate
Over the last three decades, there has been extensive interest in developing in vivo chemical sensors that can provide real-time measurements of blood gases (oxygen, carbon dioxide, and pH), glucose/lactate, and potentially other critical care analytes in the blood of hospitalized patients. However, clot formation with intravascular sensors and foreign body response toward sensors implanted subcutaneously can cause inaccurate analytical results. Further, the risk of bacterial infection from any sensor implanted in the human body is another major concern. To solve these issues, the release of an endogenous gas molecule, nitric oxide (NO), from the surface of such sensors has been investigated owing to NO`s ability to inhibit platelet activation/adhesion, foreign body response and bacterial growth. This paper summarizes the importance of NO`s therapeutic potential for this application and reviews the publications to date that report on the analytical performance of NO release sensors in laboratory testing and/or during in vivo testing.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.apmt.2017.10.002
Chinese Library Classification Number:
Citation Information:
Over the last three decades, there has been extensive interest in developing in vivo chemical sensors that can provide real-time measurements of blood gases (oxygen, carbon dioxide, and pH), glucose/lactate, and potentially other critical care analytes in the blood of hospitalized patients. However, clot formation with intravascular sensors and foreign body response toward sensors implanted subcutaneously can cause inaccurate analytical results. Further, the risk of bacterial infection from any sensor implanted in the human body is another major concern. To solve these issues, the release of an endogenous gas molecule, nitric oxide (NO), from the surface of such sensors has been investigated owing to NO`s ability to inhibit platelet activation/adhesion, foreign body response and bacterial growth. This paper summarizes the importance of NO`s therapeutic potential for this application and reviews the publications to date that report on the analytical performance of NO release sensors in laboratory testing and/or during in vivo testing.
quote
| GB/T 7714-2015 | [1] Kyoung Ha Cha, Xuewei Wang, Mark E. Meyerhoff. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.10.002. |
| MLA | [1] Kyoung Ha Cha, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.10.002. |
| APA | [1] Kyoung Ha Cha, Xuewei Wang, & Mark E. Meyerhoff. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.10.002 |
| IEEE | [1] Kyoung Ha Cha, Xuewei Wang, and Mark E. Meyerhoff, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.10.002. |