Dual-Function Self-Powered Electrochromic Batteries with Energy Storage and Display Enabled by Potential Difference AITranslate

China|University of Science and Technology of China; China|University of Science and Technology of China; Changchun Institute of Applied Chemistry; China|University of Science and Technology of China; Jilin University; China|University of Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the increasing awareness of energy savings, electrochromic smart windows with energy storage and display have attracted extensive attention. Herein, a self-powered electrochromic system (Mg ∼ PB ∼ MnO2) is initially proposed, which integrates high electrochromic performance with energy storage performance. The self-charging/discharging processes accompanied by self-coloring/bleaching processes are based on the potential difference between the electrochromic electrode and the other opposite electrodes, such as Mg or MnO2. The bleaching process is achieved by connecting the Prussian blue (PB) electrode with the Mg electrode, which releases energy. The coloring process is realized by connecting the PW electrode with the MnO2 electrode, which corresponds to the process of energy storage. In addition, the MnO2 electrode is recyclable. Due to the high potential difference between Mg and MnO2 electrodes, the system is universal and can be used for reversible cycling of various electrochromic materials, such as polyaniline (PANI) and tungsten oxide (WO3).

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02346

Chinese Library Classification Number:

Citation Information:

With the increasing awareness of energy savings, electrochromic smart windows with energy storage and display have attracted extensive attention. Herein, a self-powered electrochromic system (Mg ∼ PB ∼ MnO2) is initially proposed, which integrates high electrochromic performance with energy storage performance. The self-charging/discharging processes accompanied by self-coloring/bleaching processes are based on the potential difference between the electrochromic electrode and the other opposite electrodes, such as Mg or MnO2. The bleaching process is achieved by connecting the Prussian blue (PB) electrode with the Mg electrode, which releases energy. The coloring process is realized by connecting the PW electrode with the MnO2 electrode, which corresponds to the process of energy storage. In addition, the MnO2 electrode is recyclable. Due to the high potential difference between Mg and MnO2 electrodes, the system is universal and can be used for reversible cycling of various electrochromic materials, such as polyaniline (PANI) and tungsten oxide (WO3).

quote

GB/T 7714-2015 [1] Qian Ma, Jinxing Chen, Hui Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02346.
MLA [1] Qian Ma, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02346.
APA [1] Qian Ma, Jinxing Chen, Hui Zhang, Yuwei Su, Yujia Jiang, & Shaojun Dong. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02346
IEEE [1] Qian Ma, Jinxing Chen, Hui Zhang, Yuwei Su, Yujia Jiang, and Shaojun Dong, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02346.