daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Designer Particle Morphology to Eliminate Local Strain Accumulation in High-Nickel Layered Cathode Materials AITranslate

Liaoning University; University of Chinese Academy of Sciences; Liaoning University; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences;Beijing Polytechnic College; Harbin Institute of Technology at Weihai; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Engineering the particle morphology of high-nickel layered cathode materials is critical for tackling the instability developed in their structures upon electrochemical cycling owing to anisotropic lattice strain generated during lithium insertion/deinsertion. This study reports on the designer particle morphology of LiNi0.90Co0.05Mn0.05O2 (NCM90) cathode materials realized by processing them in pressurized oxygen atmospheres (1–10 MPa). Without conventional doping or coating, the NCM90 cathode materials exhibit a surprisingly small primary particle size and significantly increased (approximately four times) particle number at a high oxygen pressure, for example, ≥5 MPa. The NCM90 cathode materials, whose intercomparable morphological information was evaluated for the first time by deep learning, effectively eliminate the accumulation of cycling-induced local strain owing to the randomized orientation of primary particles and the homogenized distribution of small primary particles. Consequently, these cathode materials with a designer particle morphology exhibit an excellent electrical cycling performance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01272

Chinese Library Classification Number:

Citation Information:

Engineering the particle morphology of high-nickel layered cathode materials is critical for tackling the instability developed in their structures upon electrochemical cycling owing to anisotropic lattice strain generated during lithium insertion/deinsertion. This study reports on the designer particle morphology of LiNi0.90Co0.05Mn0.05O2 (NCM90) cathode materials realized by processing them in pressurized oxygen atmospheres (1–10 MPa). Without conventional doping or coating, the NCM90 cathode materials exhibit a surprisingly small primary particle size and significantly increased (approximately four times) particle number at a high oxygen pressure, for example, ≥5 MPa. The NCM90 cathode materials, whose intercomparable morphological information was evaluated for the first time by deep learning, effectively eliminate the accumulation of cycling-induced local strain owing to the randomized orientation of primary particles and the homogenized distribution of small primary particles. Consequently, these cathode materials with a designer particle morphology exhibit an excellent electrical cycling performance.

quote

GB/T 7714-2015 [1] Peng Ju, Liubin Ben, Yang Li, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01272.
MLA [1] Peng Ju, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01272.
APA [1] Peng Ju, Liubin Ben, Yang Li, Hailong Yu, Wenwu Zhao, Yuyang Chen, Yongming Zhu, & Xuejie Huang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01272
IEEE [1] Peng Ju, Liubin Ben, Yang Li, Hailong Yu, Wenwu Zhao, Yuyang Chen, Yongming Zhu, and Xuejie Huang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01272.