daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Readily Recyclable, Auto-Catalyzed Tung Oil-Derived Vitrimers and Carbon Fiber-Reinforced Composites AITranslate

Nanjing Forestry University; Nanjing Forestry University; University of Birmingham;Institute of Chemical Industry of Forest Products;Institute of Chemical Industry of Forest Products;Institute of Chemical Industry of Forest Products;Institute of Chemical Industry of Forest Products;Institute of Chemical Industry of Forest Products
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The high strength and durability of carbon fiber-reinforced composites (CFRCs) have made them a popular choice in aerospace, civil engineering, and sports equipment. However, the non-degradable resin matrix and non-destructive recycling of carbon fibers present a challenge for their sustainability. To address this issue, we have developed a new type of CFRCs that are readily recyclable and high-performing, using an auto-catalyzed tung oil-derived vitrimer and acid curing agents (TTMA) in combination with bisphenol A epoxy resin (DGEBA) or 4,4′-methylene bis (N,N-di glycidylaniline) (TGDOM). The DGEBA/TGDOM-TTMA networks contain abundant ester bonds, hydroxyl groups, and tertiary amine, which can undergo dynamic transesterification reactions (DTER) at high temperatures, leading to topological rearrangement of cross-linked networks. This results in an epoxy resin matrix with excellent mechanical properties, thermostability, and easy reprocessing, self-healing, and degradation at elevated temperatures. Moreover, the TGDOM-TTMA exhibits good stress relaxation properties due to the high concentrations of hydroxyl and tertiary amine. Additionally, we have found that carbon fibers can be completely recycled from CFRCs using ethanolamine via amidation reaction, with the recycled carbon fibers maintaining nearly 100% of the mechanical properties of the virgin samples. This study offers a sustainable and convenient strategy for designing readily recyclable and high-performance CFRCs, with important implications for the future of composite materials.

KeyWords AITranslate

tung oil recyclable autocatalyzed vitrimers degradable CFRCs
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00614

Chinese Library Classification Number:

Citation Information:

The high strength and durability of carbon fiber-reinforced composites (CFRCs) have made them a popular choice in aerospace, civil engineering, and sports equipment. However, the non-degradable resin matrix and non-destructive recycling of carbon fibers present a challenge for their sustainability. To address this issue, we have developed a new type of CFRCs that are readily recyclable and high-performing, using an auto-catalyzed tung oil-derived vitrimer and acid curing agents (TTMA) in combination with bisphenol A epoxy resin (DGEBA) or 4,4′-methylene bis (N,N-di glycidylaniline) (TGDOM). The DGEBA/TGDOM-TTMA networks contain abundant ester bonds, hydroxyl groups, and tertiary amine, which can undergo dynamic transesterification reactions (DTER) at high temperatures, leading to topological rearrangement of cross-linked networks. This results in an epoxy resin matrix with excellent mechanical properties, thermostability, and easy reprocessing, self-healing, and degradation at elevated temperatures. Moreover, the TGDOM-TTMA exhibits good stress relaxation properties due to the high concentrations of hydroxyl and tertiary amine. Additionally, we have found that carbon fibers can be completely recycled from CFRCs using ethanolamine via amidation reaction, with the recycled carbon fibers maintaining nearly 100% of the mechanical properties of the virgin samples. This study offers a sustainable and convenient strategy for designing readily recyclable and high-performance CFRCs, with important implications for the future of composite materials.

quote

GB/T 7714-2015 [1] Wenbin Li, Qianyong Chang, Laihui Xiao, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00614.
MLA [1] Wenbin Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00614.
APA [1] Wenbin Li, Qianyong Chang, Laihui Xiao, Kun Zhang, Jinrui Huang, Yigang Wang, Jie Chen, & Xiaoan Nie. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00614
IEEE [1] Wenbin Li, Qianyong Chang, Laihui Xiao, Kun Zhang, Jinrui Huang, Yigang Wang, Jie Chen, and Xiaoan Nie, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00614. keywords: {tung oil;recyclable;autocatalyzed vitrimers;degradable;CFRCs}