4D Printing of Single-Network Shape Memory Polyurethanes with Two-Way Actuation Properties AITranslate

National University of Singapore; National University of Singapore; Northwestern Polytechnical University; Institute of Materials Research and Engineering (IMRE); Institute of Materials Research and Engineering (IMRE); Institute of Materials Research and Engineering (IMRE); Northwestern Polytechnical University; National University of Singapore; National University of Singapore; Institute of Materials Research and Engineering (IMRE)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-way shape memory polymers (SMPs) have received much attention due to their ability to enable stimuli-responsive reversible structures without requiring repeated human intervention, which may be useful for application in many fields where multiple actuation cycles are desired. However, many layered or composite SMP systems are not integrated structures and suffer from several disadvantages, such as poor interlayer adhesion with limited actuation repeatability. In addition, two-way SMPs are limited by their manufacturing method to producing user-defined, complex, high-precision devices and parts. In this work, we developed a 3D-printable resin comprising two polyurethane-based oligomers with distinctly different transition temperatures─polypentadecalactone diacrylate (PPDLDA) and polycaprolactone diacrylate (PCLDA)─together with other monomers to fabricate single-network two-way shape memory smart materials by digital light projection 3D printing. The chemical, mechanical, and thermal properties of printed products can be easily tuned by facile manipulation of monomer and oligomer compositions. The PCLDA and PPDLDA switching segments were found to exhibit high mean shape fixity ratios (Rf) of >97% and high shape recovery ratios (Rr) of >89%. The strategy for achieving 3D-printable single-network two-way SMPs presented herein holds promise for applications in soft robotics, medicine, and so forth.

KeyWords AITranslate

4D printing 3D printing shape memory polymers stimuliresponsive polymers twoway actuation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01491

Chinese Library Classification Number:

Citation Information:

Two-way shape memory polymers (SMPs) have received much attention due to their ability to enable stimuli-responsive reversible structures without requiring repeated human intervention, which may be useful for application in many fields where multiple actuation cycles are desired. However, many layered or composite SMP systems are not integrated structures and suffer from several disadvantages, such as poor interlayer adhesion with limited actuation repeatability. In addition, two-way SMPs are limited by their manufacturing method to producing user-defined, complex, high-precision devices and parts. In this work, we developed a 3D-printable resin comprising two polyurethane-based oligomers with distinctly different transition temperatures─polypentadecalactone diacrylate (PPDLDA) and polycaprolactone diacrylate (PCLDA)─together with other monomers to fabricate single-network two-way shape memory smart materials by digital light projection 3D printing. The chemical, mechanical, and thermal properties of printed products can be easily tuned by facile manipulation of monomer and oligomer compositions. The PCLDA and PPDLDA switching segments were found to exhibit high mean shape fixity ratios (Rf) of >97% and high shape recovery ratios (Rr) of >89%. The strategy for achieving 3D-printable single-network two-way SMPs presented herein holds promise for applications in soft robotics, medicine, and so forth.

quote

GB/T 7714-2015 [1] Yixue Jiang, Qian Yi Leng, Yinjia Yan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01491.
MLA [1] Yixue Jiang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01491.
APA [1] Yixue Jiang, Qian Yi Leng, Yinjia Yan, Evelyn Ling Ling Ng, Heng Li Chee, Fuke Wang, Siew Yin Chan, Xian Jun Loh, John Wang, & Benjamin Qi Yu Chan. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01491
IEEE [1] Yixue Jiang, Qian Yi Leng, Yinjia Yan, Evelyn Ling Ling Ng, Heng Li Chee, Fuke Wang, Siew Yin Chan, Xian Jun Loh, John Wang, and Benjamin Qi Yu Chan, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01491. keywords: {4D printing;3D printing;shape memory polymers;stimuliresponsive polymers;twoway actuation}