Achieving Efficient Red-Emitting Sr2Ca1−δLnδWO6:Mn4+ (Ln = La, Gd, Y, Lu, δ = 0.10) Phosphors with Extraordinary Luminescence Thermal Stability for Potential UV-LEDs Application via Facile Ion Substitution in Luminescence-Ignorable Sr2CaWO6:Mn4+ AITranslate
Abstract AITranslate
In this work, we adopt a facile rare earth ions Ln3+ (Ln = La, Gd, Y, Lu) substitution strategy to achieve the efficient red luminescence Sr2Ca1−δLnδWO6:Mn4+ (δ = 0.10), which extremely improves the luminescence properties of luminescence-ignorable Sr2CaWO6:Mn4+. It is demonstrated that the substitution of Ln3+ for Ca2+ can stabilize the Mn in tetravalent state, which would like to occupy W6+ site and generate the luminescence. It is also found that the emission profile of original Sr2CaWO6:Mn4+ changes manifestly after different Ln3+ ions substitution, which is mainly attributed to the synergistic effect of lattice distortion, Mn4+ transition 2Eg → 4A2g and lattice vibration. Most fascinatingly, the Sr2Ca0.9Ln0.1WO6:0.005Mn4+ (SC0.9Ln0.1WO:0.005Mn4+, Ln = La, Gd) show extraordinary luminescence thermal stability, whose integrated emission intensity still maintains about 95% (Gd, 96.8%; La, 94.8%) at 478 K of its original value at room temperature (298 K), much better than those in most reported Mn4+-activated oxide phosphors so far. It is confirmed that the traps may play an important role for this phenomenon. Best of all, this work gives us a facile strategy to achieve efficient Mn4+-activated red-emitting materials with extraordinary luminescence thermal stabilities derived from luminescence-ignorable ones.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.0c00212
Chinese Library Classification Number:
Citation Information:
In this work, we adopt a facile rare earth ions Ln3+ (Ln = La, Gd, Y, Lu) substitution strategy to achieve the efficient red luminescence Sr2Ca1−δLnδWO6:Mn4+ (δ = 0.10), which extremely improves the luminescence properties of luminescence-ignorable Sr2CaWO6:Mn4+. It is demonstrated that the substitution of Ln3+ for Ca2+ can stabilize the Mn in tetravalent state, which would like to occupy W6+ site and generate the luminescence. It is also found that the emission profile of original Sr2CaWO6:Mn4+ changes manifestly after different Ln3+ ions substitution, which is mainly attributed to the synergistic effect of lattice distortion, Mn4+ transition 2Eg → 4A2g and lattice vibration. Most fascinatingly, the Sr2Ca0.9Ln0.1WO6:0.005Mn4+ (SC0.9Ln0.1WO:0.005Mn4+, Ln = La, Gd) show extraordinary luminescence thermal stability, whose integrated emission intensity still maintains about 95% (Gd, 96.8%; La, 94.8%) at 478 K of its original value at room temperature (298 K), much better than those in most reported Mn4+-activated oxide phosphors so far. It is confirmed that the traps may play an important role for this phenomenon. Best of all, this work gives us a facile strategy to achieve efficient Mn4+-activated red-emitting materials with extraordinary luminescence thermal stabilities derived from luminescence-ignorable ones.
quote
| GB/T 7714-2015 | [1] Kai Li, Jiaren Du, Dirk Poelman, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00212. |
| MLA | [1] Kai Li, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00212. |
| APA | [1] Kai Li, Jiaren Du, Dirk Poelman, Henk Vrielinck, Dimitrije Mara, & Rik Van Deun. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00212 |
| IEEE | [1] Kai Li, Jiaren Du, Dirk Poelman, Henk Vrielinck, Dimitrije Mara, and Rik Van Deun, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00212. |