Highly Luminescent and Stable Halide Perovskite Nanocrystals AITranslate

Nanjing University of Science and Technology; Nanjing University of Science and Technology; Nanjing University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lead halide perovskites are potential candidates for wide-color-gamut display applications. Recently, red and green light-emitting diodes (LEDs) based on these materials have achieved external quantum efficiency (EQE) of over 20%, while the blue devices lag behind them severely because of a much lower photoluminescence quantum yield (PL QY) and inferior stability. Blue perovskite nanocrystals (NCs) are promising active materials for high-efficiency devices; however, they are reported to exhibit low defect tolerance and suffer from troublesome ion migration behavior. Though some good ideas have been proposed to overcome these problems, the present results are still unsatisfactory. In this Perspective, diverse methods toward blue perovskite NCs are summarized, as well as the intrinsic origin of low stability and poor optical properties. Then, strategies to improve their performance and stability and critical challenges that severely limit the stability and performances of blue perovskite NCs are discussed. Perspectives of further developments on synthesis and applications of blue perovskite NCs are both provided.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b02100

Chinese Library Classification Number:

Citation Information:

Lead halide perovskites are potential candidates for wide-color-gamut display applications. Recently, red and green light-emitting diodes (LEDs) based on these materials have achieved external quantum efficiency (EQE) of over 20%, while the blue devices lag behind them severely because of a much lower photoluminescence quantum yield (PL QY) and inferior stability. Blue perovskite nanocrystals (NCs) are promising active materials for high-efficiency devices; however, they are reported to exhibit low defect tolerance and suffer from troublesome ion migration behavior. Though some good ideas have been proposed to overcome these problems, the present results are still unsatisfactory. In this Perspective, diverse methods toward blue perovskite NCs are summarized, as well as the intrinsic origin of low stability and poor optical properties. Then, strategies to improve their performance and stability and critical challenges that severely limit the stability and performances of blue perovskite NCs are discussed. Perspectives of further developments on synthesis and applications of blue perovskite NCs are both provided.

quote

GB/T 7714-2015 [1] Ye Wu, Xiaoming Li, Haibo Zeng. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02100.
MLA [1] Ye Wu, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02100.
APA [1] Ye Wu, Xiaoming Li, & Haibo Zeng. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02100
IEEE [1] Ye Wu, Xiaoming Li, and Haibo Zeng, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02100.