Molecular simulations of the carbon nanotubes intramolecular junctions under mechanical loading AITranslate

University of Delaware; University of Delaware; University of Delaware
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Mechanical properties of the CNTs based IMJs are extensively studied. • Stiffness of the IMJs fall within the bounds of the constituent CNTs. • Compressive failure loads of the IMJs are lower than those of the constituent CNTs. • Tensile failure load and failure modes depend on the transition region morphology. • Torsional failure load and failure modes depend on the transition region morphology. In this paper, mechanical responses of the carbon nanotubes (CNTs) intramolecular junctions (IMJs) under three generic modes of mechanical loadings – tension, compression, and torsion have been studied using molecular dynamics simulations. (5,5)-(10,0), (7,7)-(14,0), (10,10)-(20,0) armchair–zigzag and (8,0)-(6,0) zigzag–zigzag IMJs have been simulated by connecting two constituent CNTs with pentagon and heptagon rings. Classical molecular dynamics based on the velocity-Verlet algorithm has been used to solve the Newtonian equation of motion and carbon–carbon interaction in the CNT has been modeled by the Brenner potential. Mechanical properties, particularly stiffness and maximum force/torque and failure modes for different loading conditions are studied. Simulation results show that stiffness of the IMJ falls between those of the constituent CNTs. Compressive failure load of the IMJ is lower than either of the constituent CNTs. However, failure loads and damage modes of the IMJs under tensile and torsional loadings depend on the transition region in the IMJs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.10.025

Chinese Library Classification Number:

Citation Information:

Highlights • Mechanical properties of the CNTs based IMJs are extensively studied. • Stiffness of the IMJs fall within the bounds of the constituent CNTs. • Compressive failure loads of the IMJs are lower than those of the constituent CNTs. • Tensile failure load and failure modes depend on the transition region morphology. • Torsional failure load and failure modes depend on the transition region morphology. In this paper, mechanical responses of the carbon nanotubes (CNTs) intramolecular junctions (IMJs) under three generic modes of mechanical loadings – tension, compression, and torsion have been studied using molecular dynamics simulations. (5,5)-(10,0), (7,7)-(14,0), (10,10)-(20,0) armchair–zigzag and (8,0)-(6,0) zigzag–zigzag IMJs have been simulated by connecting two constituent CNTs with pentagon and heptagon rings. Classical molecular dynamics based on the velocity-Verlet algorithm has been used to solve the Newtonian equation of motion and carbon–carbon interaction in the CNT has been modeled by the Brenner potential. Mechanical properties, particularly stiffness and maximum force/torque and failure modes for different loading conditions are studied. Simulation results show that stiffness of the IMJ falls between those of the constituent CNTs. Compressive failure load of the IMJ is lower than either of the constituent CNTs. However, failure loads and damage modes of the IMJs under tensile and torsional loadings depend on the transition region in the IMJs.

quote

GB/T 7714-2015 [1] Sanjib C. Chowdhury, Bazle Z. (Gama) Haque, John W. Gillespie. Computational Materials Science, 2014(82). DOI:10.1016/j.commatsci.2013.10.025.
MLA [1] Sanjib C. Chowdhury, et al., Computational Materials Science, no. 82, 2014, https://doi.org/10.1016/j.commatsci.2013.10.025.
APA [1] Sanjib C. Chowdhury, Bazle Z. (Gama) Haque, & John W. Gillespie. (2014). Computational Materials Science(82). https://doi.org/10.1016/j.commatsci.2013.10.025
IEEE [1] Sanjib C. Chowdhury, Bazle Z. (Gama) Haque, and John W. Gillespie, Computational Materials Science, no. 82, 2014, doi: 10.1016/j.commatsci.2013.10.025.