Are Inorganic Lead Halide Perovskite Nanocrystals Promising Scintillators? AITranslate

Nanjing University of Science and Technology; Nanjing University of Science and Technology; Nanjing University of Science and Technology; Nanjing University of Science and Technology;Hangzhou TiRay Technology Co. Ltd.;Hangzhou TiRay Technology Co. Ltd.; Nanjing University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Inspections based on ionizing radiation have spread into various areas including our daily lives, industries, and scientific investigations and now face increasing demands with the development of society. Commercial X-ray detectors are mostly based on an indirect operation model in which the scintillator transforms X-ray photons into visible light and bottom photodiodes convert them into images. Obviously, the performance of the scintillator determines the final imaging properties, and the pursuit of scintillators with superior properties and lower cost is ongoing. Recently, inorganic lead halide perovskite nanocrystals (PNCs) emerged as promising scintillators for X-ray imaging. Here, we make a detailed conclusion of the superiority of PNC scintillators and take a new look at their scintillation performances. Discrepancies are discussed and some suggestions are proposed. Finally, perspectives on future developments, advice to the field, and proposed solutions to the problems toward full device performance and practical applications are provided.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00920

Chinese Library Classification Number:

Citation Information:

Inspections based on ionizing radiation have spread into various areas including our daily lives, industries, and scientific investigations and now face increasing demands with the development of society. Commercial X-ray detectors are mostly based on an indirect operation model in which the scintillator transforms X-ray photons into visible light and bottom photodiodes convert them into images. Obviously, the performance of the scintillator determines the final imaging properties, and the pursuit of scintillators with superior properties and lower cost is ongoing. Recently, inorganic lead halide perovskite nanocrystals (PNCs) emerged as promising scintillators for X-ray imaging. Here, we make a detailed conclusion of the superiority of PNC scintillators and take a new look at their scintillation performances. Discrepancies are discussed and some suggestions are proposed. Finally, perspectives on future developments, advice to the field, and proposed solutions to the problems toward full device performance and practical applications are provided.

quote

GB/T 7714-2015 [1] Xiaoming Li, Xudong Hu, Chongkang Li, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00920.
MLA [1] Xiaoming Li, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00920.
APA [1] Xiaoming Li, Xudong Hu, Chongkang Li, Wanqiu Yang, Chujie Wang, Yiyang Chen, & Haibo Zeng. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00920
IEEE [1] Xiaoming Li, Xudong Hu, Chongkang Li, Wanqiu Yang, Chujie Wang, Yiyang Chen, and Haibo Zeng, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00920.