Computational Screening of Current Collectors for Enabling Anode-Free Lithium Metal Batteries AITranslate

Carnegie Mellon University; Carnegie Mellon University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium metal cells are key for achieving high specific energy for electrification of transportation and aviation. Anode-free cells are lithium metal cells involving no excess lithium with the highest possible specific energy. In addition, anode-free cells are simpler, cheaper, and safer because they avoid the handling and manufacturing of lithium metal foils. The lack of excess lithium magnifies issues related to dendrite growth and poor cycling in anode-free cells. The electrolyte and current collector surface play a crucial role in affecting anode-free cell cycling performance. In this work, we have computationally screened for candidate current collectors that nucleate lithium effectively and allow uniform growth. These are determined by the free energy of lithium adsorption and lithium surface diffusion barrier on candidate current collectors. Using density functional theory calculations, we show that Li alloys possess ideal characteristics for Li nucleation and growth. These can lead to vastly improved performance compared to current transition-metal current collectors.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b02306

Chinese Library Classification Number:

Citation Information:

Lithium metal cells are key for achieving high specific energy for electrification of transportation and aviation. Anode-free cells are lithium metal cells involving no excess lithium with the highest possible specific energy. In addition, anode-free cells are simpler, cheaper, and safer because they avoid the handling and manufacturing of lithium metal foils. The lack of excess lithium magnifies issues related to dendrite growth and poor cycling in anode-free cells. The electrolyte and current collector surface play a crucial role in affecting anode-free cell cycling performance. In this work, we have computationally screened for candidate current collectors that nucleate lithium effectively and allow uniform growth. These are determined by the free energy of lithium adsorption and lithium surface diffusion barrier on candidate current collectors. Using density functional theory calculations, we show that Li alloys possess ideal characteristics for Li nucleation and growth. These can lead to vastly improved performance compared to current transition-metal current collectors.

quote

GB/T 7714-2015 [1] Vikram Pande, Venkatasubramanian Viswanathan. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b02306.
MLA [1] Vikram Pande, and Venkatasubramanian Viswanathan. ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b02306.
APA [1] Vikram Pande, & Venkatasubramanian Viswanathan. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b02306
IEEE [1] Vikram Pande and Venkatasubramanian Viswanathan, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b02306.