daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Surface Engineering Strategy Enables 4.5 V Sulfide-Based All-Solid-State Batteries with High Cathode Loading and Long Cycle Life AITranslate

Xiamen University; Xiamen University; University of Chinese Academy of Sciences; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; Xiamen University; University of Chinese Academy of Sciences; Xiamen University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sulfide-based all-solid-state lithium batteries (ASSLBs) with LiCoO2 (LCO) operating at high voltage (≥4.5 V vs Li+/Li) hold promise in realizing high energy density while maintaining safety. Here, we propose a solid electrolyte coating strategy to stabilize the cathode electrolyte interface and demonstrate the benefit of lithium difluoro(oxalate)borate (LiDFOB) as coating layer on the surface of Li6PS5Cl (LPSCl) to improve the performance of LCO at 4.5 V. 89.3% of initial discharge capacity can be retained after 1500 cycles at 1C (1C = 150 mA g–1). ASSLBs with high cathode loading (35.7 mg cm–2) could deliver an areal capacity over 6 mAh cm–2 (167 mAh g–1) at 0.1C and keep 85% capacity retention after 200 cycles at 0.3C. The investigation of the improvement mechanism further verifies that in situ decomposition of LiDFOB would build an (electro)chemomechanically stable interface, which not only suppresses interfacial side reactions but also buffers the cathode cracking.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01047

Chinese Library Classification Number:

Citation Information:

Sulfide-based all-solid-state lithium batteries (ASSLBs) with LiCoO2 (LCO) operating at high voltage (≥4.5 V vs Li+/Li) hold promise in realizing high energy density while maintaining safety. Here, we propose a solid electrolyte coating strategy to stabilize the cathode electrolyte interface and demonstrate the benefit of lithium difluoro(oxalate)borate (LiDFOB) as coating layer on the surface of Li6PS5Cl (LPSCl) to improve the performance of LCO at 4.5 V. 89.3% of initial discharge capacity can be retained after 1500 cycles at 1C (1C = 150 mA g–1). ASSLBs with high cathode loading (35.7 mg cm–2) could deliver an areal capacity over 6 mAh cm–2 (167 mAh g–1) at 0.1C and keep 85% capacity retention after 200 cycles at 0.3C. The investigation of the improvement mechanism further verifies that in situ decomposition of LiDFOB would build an (electro)chemomechanically stable interface, which not only suppresses interfacial side reactions but also buffers the cathode cracking.

quote

GB/T 7714-2015 [1] Kangjun Wang, Ziteng Liang, Suting Weng, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01047.
MLA [1] Kangjun Wang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01047.
APA [1] Kangjun Wang, Ziteng Liang, Suting Weng, Yu Ding, Yu Su, Yuqi Wu, Haoyue Zhong, Ang Fu, Yiou Sun, Mingzeng Luo, Jiawei Yan, Xuefeng Wang, & Yong Yang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01047
IEEE [1] Kangjun Wang, Ziteng Liang, Suting Weng, Yu Ding, Yu Su, Yuqi Wu, Haoyue Zhong, Ang Fu, Yiou Sun, Mingzeng Luo, Jiawei Yan, Xuefeng Wang, and Yong Yang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01047.