Hygroscopic MXene/Protein Nanocomposite Fibers Enabling Highly Stretchable, Antifreezing, Repairable, and Degradable Skin-Like Wearable Electronics AITranslate

University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing; University of Science and Technology Beijing
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Wearable devices made of degradable fibers are rising stars in smart healthcare by virtue of their light weight, flexibility, and weavability. Silk protein is one promising platform for ideal fiber-type electronic devices due to its inherent biocompatibility and biodegradability. However, it remains a challenge for conductive silk-based fiber electronics to achieve high stretchability and skin-like softness. Here, hygroscopic calcium-modified MXene/silk nanocomposite fibers (Ca@MSNFs) are fabricated by decorating the wet-spun MXene/silk fibers with hygroscopic CaCl2, exhibiting 3.2 g g–1 water capture capacity at 90% relative humidity (RH), high stretchability (279.9%), degradability, repairability, and freeze-resistance (−18 °C). Furthermore, the Ca@MSNFs are assembled as humidity/strain sensors to monitor respiratory signals and body movements, showing great promise for the diagnosis of apnea syndrome and rehabilitation training. Moreover, Ca@MSNFs are degradable and do not cause pollution or environmental damage. Therefore, this work offers a promising strategy for constructing stretchable and degradable electronic devices for advanced healthcare applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00397

Chinese Library Classification Number:

Citation Information:

Wearable devices made of degradable fibers are rising stars in smart healthcare by virtue of their light weight, flexibility, and weavability. Silk protein is one promising platform for ideal fiber-type electronic devices due to its inherent biocompatibility and biodegradability. However, it remains a challenge for conductive silk-based fiber electronics to achieve high stretchability and skin-like softness. Here, hygroscopic calcium-modified MXene/silk nanocomposite fibers (Ca@MSNFs) are fabricated by decorating the wet-spun MXene/silk fibers with hygroscopic CaCl2, exhibiting 3.2 g g–1 water capture capacity at 90% relative humidity (RH), high stretchability (279.9%), degradability, repairability, and freeze-resistance (−18 °C). Furthermore, the Ca@MSNFs are assembled as humidity/strain sensors to monitor respiratory signals and body movements, showing great promise for the diagnosis of apnea syndrome and rehabilitation training. Moreover, Ca@MSNFs are degradable and do not cause pollution or environmental damage. Therefore, this work offers a promising strategy for constructing stretchable and degradable electronic devices for advanced healthcare applications.

quote

GB/T 7714-2015 [1] Liancong Yue, Min Gong, Jianping Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00397.
MLA [1] Liancong Yue, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00397.
APA [1] Liancong Yue, Min Gong, Jianping Wang, Shuyue Ma, Qiuji Chen, Xiangyi Kong, Xiang Lin, Liang Zhang, Zhen Wu, & Dongrui Wang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00397
IEEE [1] Liancong Yue, Min Gong, Jianping Wang, Shuyue Ma, Qiuji Chen, Xiangyi Kong, Xiang Lin, Liang Zhang, Zhen Wu, and Dongrui Wang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00397.