Thiophene-Based Polyelectrolyte Boosts High-Performance Quasi-2D Perovskite Solar Cells with Ultralow Energy Loss AITranslate

National Taiwan University; National Taiwan University; Southern Taiwan University Science and Technology; National Taiwan University; National Taiwan University; Los Alamos National Laboratory. Los Alamos; National Taiwan University; Los Alamos National Laboratory. Los Alamos; National Taiwan University; Los Alamos National Laboratory. Los Alamos; University of California; National Taiwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The rise of quasi-2D perovskite structures holds great promise for highly efficient and stable perovskite solar cells (PCSs). As such, fabricating large-area quasi-2D perovskite solar cells (PCSs) with high power conversion remains under active exploration. We identified that maintaining the homogeneous crystalline orientation upon scaling up is a key challenge. Thus, we introduce a thiophene-based polyelectrolyte as the hole transporting layer (HTL) to facilitate large area quasi-2D PCSs fabrication with high performance. The HTL with carboxyl acid anchoring groups can be attached to various conducting metal oxide substrates, enabling a conformal self-assembled monolayer (SAM). This SAM surface facilitates the quasi-2D perovskite crystal growth vertically aligned to the substrate. Along with a favorable energy alignment, a high open-circuit voltage (VOC) of 1.24 V was achieved, approaching the Shockley-Queisser optimal limit (VOC = 1.34 V). Remarkably, the device maintained over 80% of its initial efficiency after operating at the maximum power point under simulated AM1.5G solar irradiation for 1000 h at a relative humidity of 60%. These findings offer new fabrication strategies, paving the way to scalable quasi-2D PCS production with high efficiencies.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01104

Chinese Library Classification Number:

Citation Information:

The rise of quasi-2D perovskite structures holds great promise for highly efficient and stable perovskite solar cells (PCSs). As such, fabricating large-area quasi-2D perovskite solar cells (PCSs) with high power conversion remains under active exploration. We identified that maintaining the homogeneous crystalline orientation upon scaling up is a key challenge. Thus, we introduce a thiophene-based polyelectrolyte as the hole transporting layer (HTL) to facilitate large area quasi-2D PCSs fabrication with high performance. The HTL with carboxyl acid anchoring groups can be attached to various conducting metal oxide substrates, enabling a conformal self-assembled monolayer (SAM). This SAM surface facilitates the quasi-2D perovskite crystal growth vertically aligned to the substrate. Along with a favorable energy alignment, a high open-circuit voltage (VOC) of 1.24 V was achieved, approaching the Shockley-Queisser optimal limit (VOC = 1.34 V). Remarkably, the device maintained over 80% of its initial efficiency after operating at the maximum power point under simulated AM1.5G solar irradiation for 1000 h at a relative humidity of 60%. These findings offer new fabrication strategies, paving the way to scalable quasi-2D PCS production with high efficiencies.

quote

GB/T 7714-2015 [1] HsinHsiang Huang, TsoAn Yang, LiYun Su, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01104.
MLA [1] HsinHsiang Huang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01104.
APA [1] HsinHsiang Huang, TsoAn Yang, LiYun Su, ChiungHan Chen, YuTing Chen, Dibyajyoti Ghosh, KingFu Lin, Sergei Tretiak, ChuChen Chueh, Wanyi Nie, Hsinhan Tsai, & Leeyih Wang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01104
IEEE [1] HsinHsiang Huang, TsoAn Yang, LiYun Su, ChiungHan Chen, YuTing Chen, Dibyajyoti Ghosh, KingFu Lin, Sergei Tretiak, ChuChen Chueh, Wanyi Nie, Hsinhan Tsai, and Leeyih Wang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01104.