High Dielectric Constant Polycarbonate/Nylon Multilayer Films Capacitors with Self-Healing Capability AITranslate
Abstract AITranslate
With the fast development of high-temperature metal oxide semiconductor field effect transistors for power electronics in electric vehicles, current state-of-the-art biaxially oriented polypropylene (BOPP) film capacitors need further improvement because they have a temperature rating of only 85 °C without derating the voltage to maintain a long lifetime. If a high-temperature polymer can replace BOPP without sacrificing the overall dielectric performance and cost, it is possible to remove the current water-cooling system for capacitors and significantly reduce the cost of the power electronic unit. In this work, we demonstrated new polycarbonate (PC)/nylon multilayer films (MLFs), which has a potential for even higher temperature rating because of the higher melting temperature for nylons (e.g., nylon-6). Structural and dielectric studies showed that these PC/nylon MLFs had a similar dielectric performance, such as dielectric constant, dielectric loss, and breakdown strength, as the PC/poly(vinylidene fluoride) PVDF MLFs, which were developed in the past. These PC/nylon MLFs could perform well up to 120 °C, which was limited by the glass transition temperature of PC at 145 °C. More intriguingly, packaged PC/nylon-12 MLF capacitors exhibited a self-healing capability, which had been difficult for packaged high-temperature film capacitors. Because self-healing is such a fundamental requirement for polymer film capacitors, our PC/nylon MLFs offer a potential for next-generation high-temperature and high-energy density film capacitors.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00099
Chinese Library Classification Number:
Citation Information:
With the fast development of high-temperature metal oxide semiconductor field effect transistors for power electronics in electric vehicles, current state-of-the-art biaxially oriented polypropylene (BOPP) film capacitors need further improvement because they have a temperature rating of only 85 °C without derating the voltage to maintain a long lifetime. If a high-temperature polymer can replace BOPP without sacrificing the overall dielectric performance and cost, it is possible to remove the current water-cooling system for capacitors and significantly reduce the cost of the power electronic unit. In this work, we demonstrated new polycarbonate (PC)/nylon multilayer films (MLFs), which has a potential for even higher temperature rating because of the higher melting temperature for nylons (e.g., nylon-6). Structural and dielectric studies showed that these PC/nylon MLFs had a similar dielectric performance, such as dielectric constant, dielectric loss, and breakdown strength, as the PC/poly(vinylidene fluoride) PVDF MLFs, which were developed in the past. These PC/nylon MLFs could perform well up to 120 °C, which was limited by the glass transition temperature of PC at 145 °C. More intriguingly, packaged PC/nylon-12 MLF capacitors exhibited a self-healing capability, which had been difficult for packaged high-temperature film capacitors. Because self-healing is such a fundamental requirement for polymer film capacitors, our PC/nylon MLFs offer a potential for next-generation high-temperature and high-energy density film capacitors.
quote
| GB/T 7714-2015 | [1] Zhenpeng Li, Xinyue Chen, Ci Zhang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00099. |
| MLA | [1] Zhenpeng Li, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00099. |
| APA | [1] Zhenpeng Li, Xinyue Chen, Ci Zhang, Eric Baer, Deepak Langhe, Michael Ponting, Michael Brubaker, Terry Hosking, Ruipeng Li, Masafumi Fukuto, & Lei Zhu. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00099 |
| IEEE | [1] Zhenpeng Li, Xinyue Chen, Ci Zhang, Eric Baer, Deepak Langhe, Michael Ponting, Michael Brubaker, Terry Hosking, Ruipeng Li, Masafumi Fukuto, and Lei Zhu, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00099. keywords: {multilayer films;polycarbonate;nnylons;dielectric properties;hightemperature capacitors;selfhealing} |