Computational Comparison of Late Transition Metal (100) Surfaces for the Electrocatalytic Reduction of CO to C2 Species AITranslate

Leiden University; Leiden University;Departament de Ciència de Materials i Química Fisica & Institut de Química Teòrica i Computacional (IQTCUB), Universitat de Barcelona
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This Letter compares the efficiency of the conversion of CO to C2 species (ethanol and ethylene) on nine late transition metal (100) surfaces (Co, Ni, Cu, Rh, Pd, Ag, Ir, Pt, Au) by means of reaction onset potentials calculated using density functional theory and atomistic thermodynamics. Due to adsorption–energy scaling relations, one can model trends in limiting potentials using only two descriptors, namely *C2O2 and *OH binding energies. The resulting activity plots (i) outline the binding properties of optimal catalysts, (ii) show little dependence of the overpotential on adsorption energies, especially on the weak-binding regime, and (iii) explain why Cu(100) reduces CO to ethylene at low overpotentials. Surprisingly, CO reduction to ethanol is predicted to be thermodynamically favorable on Ag(100). This points toward existing experimental results and calls for detailed studies of the conditions necessary to enhance CO electroreduction to ethanol using Ag and its alloys.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00326

Chinese Library Classification Number:

Citation Information:

This Letter compares the efficiency of the conversion of CO to C2 species (ethanol and ethylene) on nine late transition metal (100) surfaces (Co, Ni, Cu, Rh, Pd, Ag, Ir, Pt, Au) by means of reaction onset potentials calculated using density functional theory and atomistic thermodynamics. Due to adsorption–energy scaling relations, one can model trends in limiting potentials using only two descriptors, namely *C2O2 and *OH binding energies. The resulting activity plots (i) outline the binding properties of optimal catalysts, (ii) show little dependence of the overpotential on adsorption energies, especially on the weak-binding regime, and (iii) explain why Cu(100) reduces CO to ethylene at low overpotentials. Surprisingly, CO reduction to ethanol is predicted to be thermodynamically favorable on Ag(100). This points toward existing experimental results and calls for detailed studies of the conditions necessary to enhance CO electroreduction to ethanol using Ag and its alloys.

quote

GB/T 7714-2015 [1] Selwyn Hanselman, Marc T. M. Koper, Federico CalleVallejo. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00326.
MLA [1] Selwyn Hanselman, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00326.
APA [1] Selwyn Hanselman, Marc T. M. Koper, & Federico CalleVallejo. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00326
IEEE [1] Selwyn Hanselman, Marc T. M. Koper, and Federico CalleVallejo, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00326.