Boosting the Low-Temperature Performance for Li-Ion Batteries in LiPF6-Based Local High-Concentration Electrolyte AITranslate

China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; Institute of Coal Chemistry; Institute of Coal Chemistry; Institute of Coal Chemistry; Taiyuan University of Science and Technology;University of Chinese Academy of Sciences; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

LiPF6-based commercial electrolytes are widely used in lithium-ion batteries (LIBs). However, due to the low ion conductivity that originated from the high freezing point of EC, sluggish desolvation process, and large interface resistance, LIBs with the currently commercial electrolyte based on LiPF6 demonstrate unsatisfactory performance in low-temperature operation. Herein, a LiPF6-based local high-concentration electrolyte with lithium difluorobis(oxalato)phosphate (LiDFBOP) additive is designed to enhance the performance of LIBs at low temperature. Higher-concentration LiPF6 in EC-free solvent improve the overall ionic conductivity of electrolyte. The Li+–solvent–PF6– structure can be obtained to reduce the desolvation energy; meanwhile, LiDFBOP is introduced to construct an effective SEI film with high ionic conductivity and cycle stability. The graphite/Li cells demonstrate good rate performance and low-temperature performance (ca. 240 mAh g–1 at −20 °C (0.1 C)). This work provides a feasible strategy for developing a commercial LiPF6-based electrolyte to improve the operation of LIBs at low temperature.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02903

Chinese Library Classification Number:

Citation Information:

LiPF6-based commercial electrolytes are widely used in lithium-ion batteries (LIBs). However, due to the low ion conductivity that originated from the high freezing point of EC, sluggish desolvation process, and large interface resistance, LIBs with the currently commercial electrolyte based on LiPF6 demonstrate unsatisfactory performance in low-temperature operation. Herein, a LiPF6-based local high-concentration electrolyte with lithium difluorobis(oxalato)phosphate (LiDFBOP) additive is designed to enhance the performance of LIBs at low temperature. Higher-concentration LiPF6 in EC-free solvent improve the overall ionic conductivity of electrolyte. The Li+–solvent–PF6– structure can be obtained to reduce the desolvation energy; meanwhile, LiDFBOP is introduced to construct an effective SEI film with high ionic conductivity and cycle stability. The graphite/Li cells demonstrate good rate performance and low-temperature performance (ca. 240 mAh g–1 at −20 °C (0.1 C)). This work provides a feasible strategy for developing a commercial LiPF6-based electrolyte to improve the operation of LIBs at low temperature.

quote

GB/T 7714-2015 [1] Ge Song, Zonglin Yi, Fangyuan Su, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02903.
MLA [1] Ge Song, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02903.
APA [1] Ge Song, Zonglin Yi, Fangyuan Su, Lijing Xie, Zhenbing Wang, XianXian Wei, Guoning Xu, & ChengMeng Chen. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02903
IEEE [1] Ge Song, Zonglin Yi, Fangyuan Su, Lijing Xie, Zhenbing Wang, XianXian Wei, Guoning Xu, and ChengMeng Chen, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02903.