Thermochromic Multicolored Photonic Coatings with Light Polarization- and Structural Color-Dependent Changes AITranslate

Eindhoven University of Technology; Eindhoven University of Technology; Eindhoven University of Technology; South China Normal University; Eindhoven University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Both temperature-responsive and patterned photonic coatings are receiving a lot of attention from a fundamental and application point of view. However, the fabrication of multicolor patterns, which are also temperature-responsive, remains challenging. The current work presents a thermochromic photonic coating with light polarization-dependent multiple structural colors from a polymer-stabilized cholesteric liquid crystal siloxane oligomer. It is found that the structural color and the temperature response can be manipulated by varying the polymerization temperature, allowing the fabrication of thermochromic multicolor patterns. During heating, each color starts shifting at a different temperature until the sample is entirely blue at a high temperature. Upon cooling, the multicolor pattern returns, showing that the thermochromic response is reversible. On top of that, linearly polarized light dependency is also obtained, showing different reflection colors when varying the incident light polarization angles. A multicolor, thermochromic photonic coating with light polarization- and structural color-dependent features is fabricated for demonstration.

KeyWords AITranslate

cholesteric liquid crystals thermochromic linearly polarized light photonic structures 3D helical structures patterning
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01434

Chinese Library Classification Number:

Citation Information:

Both temperature-responsive and patterned photonic coatings are receiving a lot of attention from a fundamental and application point of view. However, the fabrication of multicolor patterns, which are also temperature-responsive, remains challenging. The current work presents a thermochromic photonic coating with light polarization-dependent multiple structural colors from a polymer-stabilized cholesteric liquid crystal siloxane oligomer. It is found that the structural color and the temperature response can be manipulated by varying the polymerization temperature, allowing the fabrication of thermochromic multicolor patterns. During heating, each color starts shifting at a different temperature until the sample is entirely blue at a high temperature. Upon cooling, the multicolor pattern returns, showing that the thermochromic response is reversible. On top of that, linearly polarized light dependency is also obtained, showing different reflection colors when varying the incident light polarization angles. A multicolor, thermochromic photonic coating with light polarization- and structural color-dependent features is fabricated for demonstration.

quote

GB/T 7714-2015 [1] Weixin Zhang, Albertus P.H.J. Schenning, Augustinus J.J. Kragt, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01434.
MLA [1] Weixin Zhang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01434.
APA [1] Weixin Zhang, Albertus P.H.J. Schenning, Augustinus J.J. Kragt, Guofu Zhou, & Laurens T. de Haan. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01434
IEEE [1] Weixin Zhang, Albertus P.H.J. Schenning, Augustinus J.J. Kragt, Guofu Zhou, and Laurens T. de Haan, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01434. keywords: {cholesteric liquid crystals;thermochromic;linearly polarized light;photonic structures;3D helical structures;patterning}