Transformation of Epoxidized Natural Rubber into Ionomers by Grafting of 1H-Imidazolium Ion and Development of a Dynamic Reversible Network AITranslate

Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Material Research & Development HQ, Sumitomo Rubber Industries Ltd.;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Leibniz-Institut für Polymerforschung Dresden e.V., 01069 Dresden;Institut für Textilmaschinen und Textile Hochleistungswerkstofftechnik, Technische Universität Dresden; Germany|Tampere University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Epoxidized natural rubber (ENR) was grafted with imidazolium ions, giving the materials self-healing and reprocessing properties. These imidazolium ions in the form of neutral ionic repeating units transformed the polyisoprene-based polymer chains into ionomers. Fourier transform infrared (FTIR) spectroscopy and solid-state nuclear magnetic resonance (NMR) analyses were carried out to confirm various interactions between ENR and 1H-imidazole. In particular, dynamic hydrogen bonding and the formation of ionic aggregates led to superior mechanical strength (tensile strength, ∼4.5 MPa; elongation at break, ∼700%), self-healing efficiency (90% in terms of elongation), and reprocessability of the resulting compound. Furthermore, the material exhibited excellent transparency with a normalized transparency of 90 ± 0.7% at a typical thickness of 0.5 mm. The visualization and the stability of the healing processes were confirmed by scanning electron microscopy (SEM) and confocal microscopy analyses. Finally, temperature scanning stress relaxation (TSSR) studies were carried out to identify the different types of stress relaxation behavior of the material and the effects of various noncovalent interactions on the high-temperature stability of the compounds. These studies could assist to gain significant insight into natural rubber-based advanced materials for sustainable development.

KeyWords AITranslate

epoxidized natural rubber 1Himidazole selfhealing reprocessing dynamic reversible networks
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00976

Chinese Library Classification Number:

Citation Information:

Epoxidized natural rubber (ENR) was grafted with imidazolium ions, giving the materials self-healing and reprocessing properties. These imidazolium ions in the form of neutral ionic repeating units transformed the polyisoprene-based polymer chains into ionomers. Fourier transform infrared (FTIR) spectroscopy and solid-state nuclear magnetic resonance (NMR) analyses were carried out to confirm various interactions between ENR and 1H-imidazole. In particular, dynamic hydrogen bonding and the formation of ionic aggregates led to superior mechanical strength (tensile strength, ∼4.5 MPa; elongation at break, ∼700%), self-healing efficiency (90% in terms of elongation), and reprocessability of the resulting compound. Furthermore, the material exhibited excellent transparency with a normalized transparency of 90 ± 0.7% at a typical thickness of 0.5 mm. The visualization and the stability of the healing processes were confirmed by scanning electron microscopy (SEM) and confocal microscopy analyses. Finally, temperature scanning stress relaxation (TSSR) studies were carried out to identify the different types of stress relaxation behavior of the material and the effects of various noncovalent interactions on the high-temperature stability of the compounds. These studies could assist to gain significant insight into natural rubber-based advanced materials for sustainable development.

quote

GB/T 7714-2015 [1] Subhradeep Mandal, Sakrit Hait, Frank Simon, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00976.
MLA [1] Subhradeep Mandal, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00976.
APA [1] Subhradeep Mandal, Sakrit Hait, Frank Simon, Anik Ghosh, Ulrich Scheler, Injamamul Arief, Toshio Tada, Tung X. Hoang, Sven Wießner, Gert Heinrich, & Amit Das. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00976
IEEE [1] Subhradeep Mandal, Sakrit Hait, Frank Simon, Anik Ghosh, Ulrich Scheler, Injamamul Arief, Toshio Tada, Tung X. Hoang, Sven Wießner, Gert Heinrich, and Amit Das, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00976. keywords: {epoxidized natural rubber;1Himidazole;selfhealing;reprocessing;dynamic reversible networks}