Interphases and Electrode Crosstalk Dictate the Thermal Stability of Solid-State Batteries AITranslate

Purdue University; Purdue University; Purdue University; Purdue University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Solid-state batteries, because of their high energy density, are promising candidates for long-range electric vehicles and electric aviation. While the enhanced safety potential of solid-state batteries has been typically ascribed to the nonflammability of solid electrolytes, an extensive interrogation of their thermal stability is still required. In this work, we reveal how the thermal stability in sulfide-based solid-state batteries is critically dependent on the interphase interactions at the solid electrolyte/Li interface, thereby illustrating the drastically different thermal signature of Li10SnP2S12 when compared with Li3PS4 and Li6PS5Cl. Our study shows that thermal runaway occurs even for a pristine Li10SnP2S12/Li interface and is severely exacerbated with cycling, which exhibits a massive thermal spike at the melting point of Li; this shift in thermal response uniquely correlates to the Li10SnP2S12 interphase evolution. On the basis of these distinct thermal signatures, cell-level mechanistic safety maps cognizant of the Li/interphase interaction, cathode/Li crosstalk, and specific energy are delineated.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02443

Chinese Library Classification Number:

Citation Information:

Solid-state batteries, because of their high energy density, are promising candidates for long-range electric vehicles and electric aviation. While the enhanced safety potential of solid-state batteries has been typically ascribed to the nonflammability of solid electrolytes, an extensive interrogation of their thermal stability is still required. In this work, we reveal how the thermal stability in sulfide-based solid-state batteries is critically dependent on the interphase interactions at the solid electrolyte/Li interface, thereby illustrating the drastically different thermal signature of Li10SnP2S12 when compared with Li3PS4 and Li6PS5Cl. Our study shows that thermal runaway occurs even for a pristine Li10SnP2S12/Li interface and is severely exacerbated with cycling, which exhibits a massive thermal spike at the melting point of Li; this shift in thermal response uniquely correlates to the Li10SnP2S12 interphase evolution. On the basis of these distinct thermal signatures, cell-level mechanistic safety maps cognizant of the Li/interphase interaction, cathode/Li crosstalk, and specific energy are delineated.

quote

GB/T 7714-2015 [1] Bairav S. Vishnugopi, Md Toukir Hasan, Hanwei Zhou, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02443.
MLA [1] Bairav S. Vishnugopi, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02443.
APA [1] Bairav S. Vishnugopi, Md Toukir Hasan, Hanwei Zhou, & Partha P. Mukherjee. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02443
IEEE [1] Bairav S. Vishnugopi, Md Toukir Hasan, Hanwei Zhou, and Partha P. Mukherjee, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02443.