A Versatile Li0.5FePO4 Reference Electrode for Nonaqueous Electrochemical Conversion Technologies AITranslate

Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University; Stanford University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The electrification of chemical processes provides a means to effectively utilize rapidly expanding renewable energy resources. Nonaqueous electrochemical systems offer promising opportunities, such as steering selectivity toward N2 reduction over the H2 evolution reaction. However, nonaqueous environments pose challenges for reference electrodes (REs), presenting a need for their design and development. In this study, we show the utility of a Li0.5FePO4 (LFP) RE for nonaqueous electrochemical systems, demonstrating various desirable characteristics: remarkable voltage stability across a variety of electrochemical environments, geometric flexibility, and minimal cation leakage concerns. We show that the LFP RE can serve as an immediate replacement for conventional REs commonly employed in nonaqueous electrochemical systems, such as Pt wire and Ag/AgCl REs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02190

Chinese Library Classification Number:

Citation Information:

The electrification of chemical processes provides a means to effectively utilize rapidly expanding renewable energy resources. Nonaqueous electrochemical systems offer promising opportunities, such as steering selectivity toward N2 reduction over the H2 evolution reaction. However, nonaqueous environments pose challenges for reference electrodes (REs), presenting a need for their design and development. In this study, we show the utility of a Li0.5FePO4 (LFP) RE for nonaqueous electrochemical systems, demonstrating various desirable characteristics: remarkable voltage stability across a variety of electrochemical environments, geometric flexibility, and minimal cation leakage concerns. We show that the LFP RE can serve as an immediate replacement for conventional REs commonly employed in nonaqueous electrochemical systems, such as Pt wire and Ag/AgCl REs.

quote

GB/T 7714-2015 [1] Eric J. McShane, Peter Benedek, Valerie A. Niemann, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02190.
MLA [1] Eric J. McShane, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02190.
APA [1] Eric J. McShane, Peter Benedek, Valerie A. Niemann, Sarah J. Blair, Gaurav A. Kamat, Adam C. Nielander, Thomas F. Jaramillo, & Matteo Cargnello. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02190
IEEE [1] Eric J. McShane, Peter Benedek, Valerie A. Niemann, Sarah J. Blair, Gaurav A. Kamat, Adam C. Nielander, Thomas F. Jaramillo, and Matteo Cargnello, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02190.