Full Exclusion of Branched Hexanes from Their Linear Isomer by a Robust Aluminum Metal–Organic Framework with Tailored Pore Structure AITranslate

South China University of Technology; Wake Forest University; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; Wake Forest University;Hoffmann Institute of Advanced Materials
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High-efficiency separation of hexane isomers through selective molecular exclusion represents an important yet challenging task in the petrochemical industry. It has stringent requirements on the adsorbents’ pore shape and dimensions. Here we report the complete exclusion of branched hexanes from their linear isomer by an aluminum metal–organic framework, CAU-21-ODB (ODB = 4,4′-oxidibenzoate) with high stability. The unique gourd-shaped channels with suitable pore aperture lead to substantial uptake of nHEX (141 mg/g at 30 °C) but negligible adsorption of its branched isomers under identical conditions. The capability of CAU-21-ODB for the separation of hexane isomers has been verified by multicomponent breakthrough experiments. DFT calculations further confirm the size-exclusion-based separation mechanism.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00282

Chinese Library Classification Number:

Citation Information:

High-efficiency separation of hexane isomers through selective molecular exclusion represents an important yet challenging task in the petrochemical industry. It has stringent requirements on the adsorbents’ pore shape and dimensions. Here we report the complete exclusion of branched hexanes from their linear isomer by an aluminum metal–organic framework, CAU-21-ODB (ODB = 4,4′-oxidibenzoate) with high stability. The unique gourd-shaped channels with suitable pore aperture lead to substantial uptake of nHEX (141 mg/g at 30 °C) but negligible adsorption of its branched isomers under identical conditions. The capability of CAU-21-ODB for the separation of hexane isomers has been verified by multicomponent breakthrough experiments. DFT calculations further confirm the size-exclusion-based separation mechanism.

quote

GB/T 7714-2015 [1] Liang Yu, Saif Ullah, Jinze Yao, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00282.
MLA [1] Liang Yu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00282.
APA [1] Liang Yu, Saif Ullah, Jinze Yao, Danxia Lin, Jiajin Huang, Shi Tu, Haoyuan Luo, Qibin Xia, Timo Thonhauser, & Hao Wang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00282
IEEE [1] Liang Yu, Saif Ullah, Jinze Yao, Danxia Lin, Jiajin Huang, Shi Tu, Haoyuan Luo, Qibin Xia, Timo Thonhauser, and Hao Wang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00282.