A Kinetic Indicator of Ultrafast Nickel-Rich Layered Oxide Cathodes AITranslate
Abstract AITranslate
Elucidating high-rate cycling-induced nonequilibrium electrode reactions is crucial for developing extreme fast charging (XFC) batteries. Herein, we unveiled the distinct rate capabilities of a series of Ni-rich layered oxide (NRLO) cathodes by quantitatively establishing their dynamic structure–kinetics relationships. Contrary to conventional views, we discovered electrode kinetic properties obtained ex-situ near equilibrium states failed to assess the effective rate capability of NRLOs at ultrafast C rates. Further, the kinetic phase heterogeneity, characterized by the dynamic separations in in-situ X-ray diffraction patterns and deviations in NRLO c-axis lattice parameters, exclusively correlated with the capacity reduction under XFC and became an effective indicator of the NRLO rate capability. Enhancing the cycling temperature boosted the rate capability of studied NRLOs by ∼10%, which was further verified to mitigate the kinetic phase heterogeneity during XFC. Overall, this study lays the groundwork for tuning the kinetic phase heterogeneity of electrodes to develop ultrafast batteries.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00513
Chinese Library Classification Number:
Citation Information:
Elucidating high-rate cycling-induced nonequilibrium electrode reactions is crucial for developing extreme fast charging (XFC) batteries. Herein, we unveiled the distinct rate capabilities of a series of Ni-rich layered oxide (NRLO) cathodes by quantitatively establishing their dynamic structure–kinetics relationships. Contrary to conventional views, we discovered electrode kinetic properties obtained ex-situ near equilibrium states failed to assess the effective rate capability of NRLOs at ultrafast C rates. Further, the kinetic phase heterogeneity, characterized by the dynamic separations in in-situ X-ray diffraction patterns and deviations in NRLO c-axis lattice parameters, exclusively correlated with the capacity reduction under XFC and became an effective indicator of the NRLO rate capability. Enhancing the cycling temperature boosted the rate capability of studied NRLOs by ∼10%, which was further verified to mitigate the kinetic phase heterogeneity during XFC. Overall, this study lays the groundwork for tuning the kinetic phase heterogeneity of electrodes to develop ultrafast batteries.
quote
| GB/T 7714-2015 | [1] Jian Wang, Hyejeong Hyun, Sungjae Seo, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00513. |
| MLA | [1] Jian Wang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00513. |
| APA | [1] Jian Wang, Hyejeong Hyun, Sungjae Seo, Kyeongjae Jeong, Jeongwoo Han, Sugeun Jo, Hwiho Kim, Bonho Koo, Donggun Eum, Juwon Kim, Jinkyu Chung, HoonHwe Cho, Heung Nam Han, Tae Joo Shin, Meng Ni, Kisuk Kang, & Jongwoo Lim. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00513 |
| IEEE | [1] Jian Wang, Hyejeong Hyun, Sungjae Seo, Kyeongjae Jeong, Jeongwoo Han, Sugeun Jo, Hwiho Kim, Bonho Koo, Donggun Eum, Juwon Kim, Jinkyu Chung, HoonHwe Cho, Heung Nam Han, Tae Joo Shin, Meng Ni, Kisuk Kang, and Jongwoo Lim, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00513. |