Highly Sensitive Flexible Temperature Sensor Made Using PEDOT:PSS/PANI AITranslate
Abstract AITranslate
This work proposes a design, fabrication, and characterization of flexible temperature sensors using temperature-sensitive materials, which are applied using a drop coating method. Temperature-sensitive materials were fabricated by mixing poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) with polyaniline (PEDOT:PSS/PANI). The temperature coefficient of resistance reached −0.803%/°C. Moreover, the detection resolution reached 0.1 °C and had a fast response time of 200 ms. In addition, the sensor can sense spatial temperatures. The sensor has the advantages of low cost, a simple preparation process, and the potential to be used in medical rehabilitation and early disease prevention.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01224
Chinese Library Classification Number:
Citation Information:
This work proposes a design, fabrication, and characterization of flexible temperature sensors using temperature-sensitive materials, which are applied using a drop coating method. Temperature-sensitive materials were fabricated by mixing poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) with polyaniline (PEDOT:PSS/PANI). The temperature coefficient of resistance reached −0.803%/°C. Moreover, the detection resolution reached 0.1 °C and had a fast response time of 200 ms. In addition, the sensor can sense spatial temperatures. The sensor has the advantages of low cost, a simple preparation process, and the potential to be used in medical rehabilitation and early disease prevention.
quote
| GB/T 7714-2015 | [1] Juncai Song, Yuan Wei, Manzhang Xu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01224. |
| MLA | [1] Juncai Song, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01224. |
| APA | [1] Juncai Song, Yuan Wei, Manzhang Xu, Jiuwei Gao, Lei Luo, Hao Wu, Xingji Li, Yue Li, & Xuewen Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01224 |
| IEEE | [1] Juncai Song, Yuan Wei, Manzhang Xu, Jiuwei Gao, Lei Luo, Hao Wu, Xingji Li, Yue Li, and Xuewen Wang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01224. keywords: {flexible temperature sensor;temperature;temperature coefficient of resistance (TCR);response time;detection resolution} |