Numerical study of the effect of prior deformation history on texture evolution during equal channel angular pressing AITranslate

National Research Laboratory for Computer Aided Materials Processing; Institute of Technology;National Research Laboratory for Computer Aided Materials Processing;National Research Laboratory for Computer Aided Materials Processing; Kookmin University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • The effect of initial textures on texture evolution during the ECAP is investigated. • Heterogeneity of textures in routes A and C up to four passes is studied. • Simulations are made by finite element analyses with the FC Taylor model. • The initial texture originated from extrusion gets mixed up with the shear texture. • The rolling initial texture yields strong development of the rotated shear texture. It is experimentally well known that mechanical properties of the material depend on crystallographic texture distribution which varies depending on deformation history. When the material deforms at several stages, it is not easy to follow up the effect of prior deformation on the final texture of the material. In the present study, the effect of deformation history on texture evolution during equal channel angular pressing (ECAP) of FCC polycrystalline metal like AA1050 is investigated by the finite element method and polycrystal plasticity model based on full constraints Taylor model. The texture evolution during the multi-pass ECAP is simulated with the initial textures determined by three virtual specimens prepared by the fully annealed, extruded, and flat-rolled materials. By comparing the pole figures and orientation distribution functions, the effect of prior deformation histories on the texture evolution is numerically studied according to the routes A and C up to four passes across the thickness of the specimen. For the extruded specimen, it is not enough to wipe out the trace of the initial textures originated from the extrusion even after four passes. For the rolled specimen, strong development of the rotated simple shear texture readily occurred with the rotation about the transverse direction of the ECAP die. This study indicates that it is necessary to control the initial texture properly for achieving a desired mechanical property.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2013.05.034

Chinese Library Classification Number:

Citation Information:

Highlights • The effect of initial textures on texture evolution during the ECAP is investigated. • Heterogeneity of textures in routes A and C up to four passes is studied. • Simulations are made by finite element analyses with the FC Taylor model. • The initial texture originated from extrusion gets mixed up with the shear texture. • The rolling initial texture yields strong development of the rotated shear texture. It is experimentally well known that mechanical properties of the material depend on crystallographic texture distribution which varies depending on deformation history. When the material deforms at several stages, it is not easy to follow up the effect of prior deformation on the final texture of the material. In the present study, the effect of deformation history on texture evolution during equal channel angular pressing (ECAP) of FCC polycrystalline metal like AA1050 is investigated by the finite element method and polycrystal plasticity model based on full constraints Taylor model. The texture evolution during the multi-pass ECAP is simulated with the initial textures determined by three virtual specimens prepared by the fully annealed, extruded, and flat-rolled materials. By comparing the pole figures and orientation distribution functions, the effect of prior deformation histories on the texture evolution is numerically studied according to the routes A and C up to four passes across the thickness of the specimen. For the extruded specimen, it is not enough to wipe out the trace of the initial textures originated from the extrusion even after four passes. For the rolled specimen, strong development of the rotated simple shear texture readily occurred with the rotation about the transverse direction of the ECAP die. This study indicates that it is necessary to control the initial texture properly for achieving a desired mechanical property.

quote

GB/T 7714-2015 [1] DongKyu Kim, KyungHwan Jung, WonWoong Park, et al. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.05.034.
MLA [1] DongKyu Kim, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.05.034.
APA [1] DongKyu Kim, KyungHwan Jung, WonWoong Park, YongTaek Im, & YongShin Lee. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.05.034
IEEE [1] DongKyu Kim, KyungHwan Jung, WonWoong Park, YongTaek Im, and YongShin Lee, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.05.034.