Thermodynamic assessments of the Ni–Pt and Al–Ni–Pt systems AITranslate
Abstract AITranslate
The Ni–Pt system is assessed using the CALPHAD method. The four fcc-based phases, i.e. disordered solid solution phase, Ni3Pt–L12, NiPt–L10 and NiPt3–L12, are described by a four-sublattice model. The calculated thermodynamic properties and order/disorder phase transformations are in good agreement with the experimental data. In order to facilitate the assessment, first-principles pseudopotential calculations are also performed to calculate the enthalpy of formation at 0 K, and comparison with the assessed values is discussed. By combining the assessments of Al–Ni and Al–Pt, the Al–Ni–Pt ternary system is assessed within a narrow temperature range, focusing on the fcc-based phases and their phase equilibria with B2 phase.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2009.06.002
Chinese Library Classification Number:
Citation Information:
The Ni–Pt system is assessed using the CALPHAD method. The four fcc-based phases, i.e. disordered solid solution phase, Ni3Pt–L12, NiPt–L10 and NiPt3–L12, are described by a four-sublattice model. The calculated thermodynamic properties and order/disorder phase transformations are in good agreement with the experimental data. In order to facilitate the assessment, first-principles pseudopotential calculations are also performed to calculate the enthalpy of formation at 0 K, and comparison with the assessed values is discussed. By combining the assessments of Al–Ni and Al–Pt, the Al–Ni–Pt ternary system is assessed within a narrow temperature range, focusing on the fcc-based phases and their phase equilibria with B2 phase.
quote
| GB/T 7714-2015 | [1] XiaoGang Lu, Bo Sundman, John A˚gren. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.06.002. |
| MLA | [1] XiaoGang Lu, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.06.002. |
| APA | [1] XiaoGang Lu, Bo Sundman, & John A˚gren. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.06.002 |