daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Monodisperse Styrene-Maleic Anhydride-Isoprene Terpolymer Microspheres with Tunable Crosslinking Density Prepared by Self-Stabilized Precipitation Polymerization AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Synthesis and industrial production of functional monodisperse microspheres still face enormous challenges like precise size control and process simplification. Herein, a strategy to prepare monodisperse styrene-maleic anhydride-isoprene terpolymer microspheres via self-stabilized precipitation polymerization was reported. The prepared microspheres with different isoprene proportions have uniform particle sizes (623–1156 nm) and narrow size distributions. The structure analysis showed that the copolymerization proceeded in an alternating way between the electron donor (styrene and isoprene) and electron acceptor (maleic anhydride) monomer, and isoprene was incorporated into the polymer chain through 1, 4 addition. The gel fraction of microspheres varies from 0 to 99% along with an increasing isoprene feeding ratio. The Diels–Alder (D–A) reaction between maleic anhydride and isoprene can be effectively inhibited by increasing the amount of initiator or decreasing the polymerization temperature. The resultant uniform microspheres contain reactive anhydride groups and unsaturated C═C bonds derived from isoprene, which can be used to covalently attach functional moieties and have great potential in fields of adsorption and separation, drug delivery, biodetection, and enzyme immobilization.

KeyWords AITranslate

monodisperse microspheres terpolymerization tunable crosslinking density maleic anhydride isoprene
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01156

Chinese Library Classification Number:

Citation Information:

Synthesis and industrial production of functional monodisperse microspheres still face enormous challenges like precise size control and process simplification. Herein, a strategy to prepare monodisperse styrene-maleic anhydride-isoprene terpolymer microspheres via self-stabilized precipitation polymerization was reported. The prepared microspheres with different isoprene proportions have uniform particle sizes (623–1156 nm) and narrow size distributions. The structure analysis showed that the copolymerization proceeded in an alternating way between the electron donor (styrene and isoprene) and electron acceptor (maleic anhydride) monomer, and isoprene was incorporated into the polymer chain through 1, 4 addition. The gel fraction of microspheres varies from 0 to 99% along with an increasing isoprene feeding ratio. The Diels–Alder (D–A) reaction between maleic anhydride and isoprene can be effectively inhibited by increasing the amount of initiator or decreasing the polymerization temperature. The resultant uniform microspheres contain reactive anhydride groups and unsaturated C═C bonds derived from isoprene, which can be used to covalently attach functional moieties and have great potential in fields of adsorption and separation, drug delivery, biodetection, and enzyme immobilization.

quote

GB/T 7714-2015 [1] Can Xu, Chuxuan Chen, Jing Jiang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01156.
MLA [1] Can Xu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01156.
APA [1] Can Xu, Chuxuan Chen, Jing Jiang, Changwen Zhao, Yuhong Ma, & Wantai Yang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01156
IEEE [1] Can Xu, Chuxuan Chen, Jing Jiang, Changwen Zhao, Yuhong Ma, and Wantai Yang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01156. keywords: {monodisperse microspheres;terpolymerization;tunable crosslinking density;maleic anhydride;isoprene}