Modelling of hot cracking in welding with a cellular automaton combined with an intergranular fluid flow model AITranslate
Abstract AITranslate
Highlights • Hot cracking is investigated in heterogeneous fields induced by welding. • Liquid films are predicted based on a cellular automaton. • Effects of strain localization and solidification shrinkage are compared. • Depression in liquid films at grain boundaries indicates possible pore nucleation. Hot cracking phenomena in welds are still a major issue to choose suitable welding conditions. Solidification cracking in welds depends on microstructure morphology, thermal and mechanical loadings. It is still difficult to discriminate the influence of the different phenomena because they are all connected. To investigate solidification cracking, numerical modelling that integrates most of these phenomena is developed in this paper. Thermal and mechanical fields are computed with a finite element model at the process scale. The thermal field is combined with a cellular automaton (CA) to predict microstructure at a mesoscale. Based, on this prediction, the intergranular network is extracted. Finally, the pressure in the intergranular fluid network is computed during solidification. The fluid flow model along grain boundaries predicts an eventual nucleation of pore/void in the remaining liquid by investigating the maximum pressure drop in the solidifying microstructure. The numerical model is able to describe some hot cracking phenomena observed during experimental tests.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2013.09.067
Chinese Library Classification Number:
Citation Information:
Highlights • Hot cracking is investigated in heterogeneous fields induced by welding. • Liquid films are predicted based on a cellular automaton. • Effects of strain localization and solidification shrinkage are compared. • Depression in liquid films at grain boundaries indicates possible pore nucleation. Hot cracking phenomena in welds are still a major issue to choose suitable welding conditions. Solidification cracking in welds depends on microstructure morphology, thermal and mechanical loadings. It is still difficult to discriminate the influence of the different phenomena because they are all connected. To investigate solidification cracking, numerical modelling that integrates most of these phenomena is developed in this paper. Thermal and mechanical fields are computed with a finite element model at the process scale. The thermal field is combined with a cellular automaton (CA) to predict microstructure at a mesoscale. Based, on this prediction, the intergranular network is extracted. Finally, the pressure in the intergranular fluid network is computed during solidification. The fluid flow model along grain boundaries predicts an eventual nucleation of pore/void in the remaining liquid by investigating the maximum pressure drop in the solidifying microstructure. The numerical model is able to describe some hot cracking phenomena observed during experimental tests.
quote
| GB/T 7714-2015 | [1] Cyril Bordreuil, Aurélie Niel. Computational Materials Science, 2014(82). DOI:10.1016/j.commatsci.2013.09.067. |
| MLA | [1] Cyril Bordreuil, and Aurélie Niel. Computational Materials Science, no. 82, 2014, https://doi.org/10.1016/j.commatsci.2013.09.067. |
| APA | [1] Cyril Bordreuil, & Aurélie Niel. (2014). Computational Materials Science(82). https://doi.org/10.1016/j.commatsci.2013.09.067 |