Exploring Different Carbon Allotrope Thermoplastic Composites for Electrochemical Sensing AITranslate
Abstract AITranslate
Composite electrodes are an effective and cheap way to utilize a wide range of carbon materials to make electrodes. More recently, thermoplastics have been widely used as the binder to make carbon composite electrodes, as varying fabrication approaches, such as three-dimensional (3D) printing, can make highly reproducible electrodes. However, there is a clear need to understand how the electrochemical performance of different carbon allotrope materials varies when made into sensors. We accessed poly(lactic acid) (PLA) thermoplastic filaments containing carbon black, graphite, graphene, multiwall carbon nanotube (MWCNT), and carbon fiber using various electrochemical techniques. Graphite/PLA and graphene/PLA electrodes showed the best electron transfer kinetics. Graphene/PLA electrodes had the greatest sensitivity and lowest limit of detection for the measurement of serotonin. CB/PLA was least prone to electrode fouling from oxidative by-product generated from the oxidation of serotonin. 3D printing was used to make various carbon allotrope materials into complex shapes to evaluate the batch uniformity of the printed parts. Of all the materials explored, CB/PLA had the best resolution and batch uniformity when compared with PLA. Overall, our study highlights that the type of carbon allotrope has as much influence as the amount of carbon on the electrochemical performance of carbon thermoplastic electrodes. These findings will provide significant guidance on the appropriate choice of carbon thermoplastic composite materials when designing electrodes for a wide range of applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c00349
Chinese Library Classification Number:
Citation Information:
Composite electrodes are an effective and cheap way to utilize a wide range of carbon materials to make electrodes. More recently, thermoplastics have been widely used as the binder to make carbon composite electrodes, as varying fabrication approaches, such as three-dimensional (3D) printing, can make highly reproducible electrodes. However, there is a clear need to understand how the electrochemical performance of different carbon allotrope materials varies when made into sensors. We accessed poly(lactic acid) (PLA) thermoplastic filaments containing carbon black, graphite, graphene, multiwall carbon nanotube (MWCNT), and carbon fiber using various electrochemical techniques. Graphite/PLA and graphene/PLA electrodes showed the best electron transfer kinetics. Graphene/PLA electrodes had the greatest sensitivity and lowest limit of detection for the measurement of serotonin. CB/PLA was least prone to electrode fouling from oxidative by-product generated from the oxidation of serotonin. 3D printing was used to make various carbon allotrope materials into complex shapes to evaluate the batch uniformity of the printed parts. Of all the materials explored, CB/PLA had the best resolution and batch uniformity when compared with PLA. Overall, our study highlights that the type of carbon allotrope has as much influence as the amount of carbon on the electrochemical performance of carbon thermoplastic electrodes. These findings will provide significant guidance on the appropriate choice of carbon thermoplastic composite materials when designing electrodes for a wide range of applications.
quote
| GB/T 7714-2015 | [1] Khalil K. Hussain, Ricoveer Singh Shergill, Hairul Hisham Hamzah, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00349. |
| MLA | [1] Khalil K. Hussain, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00349. |
| APA | [1] Khalil K. Hussain, Ricoveer Singh Shergill, Hairul Hisham Hamzah, Mark S. Yeoman, & Bhavik A. Patel. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00349 |
| IEEE | [1] Khalil K. Hussain, Ricoveer Singh Shergill, Hairul Hisham Hamzah, Mark S. Yeoman, and Bhavik A. Patel, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00349. keywords: {carbon thermoplastic;carbon allotropes;3D printing;electrochemical sensors;serotonin} |