Direct Synthesis of Quaternary Alkylammonium-Capped Perovskite Nanocrystals for Efficient Blue and Green Light-Emitting Diodes AITranslate

Switzerland|Institute of Inorganic Chemistry; Switzerland|Institute of Inorganic Chemistry; Switzerland|Institute of Inorganic Chemistry; Switzerland|Institute of Inorganic Chemistry; Switzerland|Institute of Inorganic Chemistry; Switzerland|Institute of Inorganic Chemistry; Switzerland|Institute of Inorganic Chemistry
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Cesium lead halide nanocrystals (CsPbX3 NCs) are new inorganic light sources covering the entire visible spectral range and exhibiting near-unity efficiencies. While the last years have seen rapid progress in green and red electroluminescence from CsPbX3 NCs, the development of blue counterparts remained rather stagnant. Controlling the surface state of CsPbX3 NCs had proven to be a major factor governing the efficiency of the charge injection and for diminishing the density of traps. Although didodecyldimethylammonium halides (DDAX; X = Br, Cl) had been known to improve the luminescence of CsPbX3 NCs when applied postsynthetically, they had not been used as the sole long-chain ammonium ligand directly in the synthesis of these NCs. Herein we report a facile, direct synthesis of DDAX-stabilized CsPbX3 NCs. We then demonstrate blue and green light-emitting diodes, characterized by the electroluminescence at 463–515 nm and external quantum efficiencies of 9.80% for green, 4.96% for sky-blue, and 1.03% for deep-blue spectral regions.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01915

Chinese Library Classification Number:

Citation Information:

Cesium lead halide nanocrystals (CsPbX3 NCs) are new inorganic light sources covering the entire visible spectral range and exhibiting near-unity efficiencies. While the last years have seen rapid progress in green and red electroluminescence from CsPbX3 NCs, the development of blue counterparts remained rather stagnant. Controlling the surface state of CsPbX3 NCs had proven to be a major factor governing the efficiency of the charge injection and for diminishing the density of traps. Although didodecyldimethylammonium halides (DDAX; X = Br, Cl) had been known to improve the luminescence of CsPbX3 NCs when applied postsynthetically, they had not been used as the sole long-chain ammonium ligand directly in the synthesis of these NCs. Herein we report a facile, direct synthesis of DDAX-stabilized CsPbX3 NCs. We then demonstrate blue and green light-emitting diodes, characterized by the electroluminescence at 463–515 nm and external quantum efficiencies of 9.80% for green, 4.96% for sky-blue, and 1.03% for deep-blue spectral regions.

quote

GB/T 7714-2015 [1] Yevhen Shynkarenko, Maryna I. Bodnarchuk, Caterina Bernasconi, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01915.
MLA [1] Yevhen Shynkarenko, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01915.
APA [1] Yevhen Shynkarenko, Maryna I. Bodnarchuk, Caterina Bernasconi, Yuliia Berezovska, Vladyslav Verteletskyi, Stefan T. Ochsenbein, & Maksym V. Kovalenko. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01915
IEEE [1] Yevhen Shynkarenko, Maryna I. Bodnarchuk, Caterina Bernasconi, Yuliia Berezovska, Vladyslav Verteletskyi, Stefan T. Ochsenbein, and Maksym V. Kovalenko, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01915.